Physical Properties Metric English Comments
Thickness 30.0 - 150 microns
1.18 - 5.91 mil
Recommended
Polimeri Europa Greenflex® FF 35 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FF 35 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. The resin shows good strechability and sealability.Main Applications: Greenflex FF 35 is suitable for flexibl..
Thickness 30.0 - 150 microns
1.18 - 5.91 mil
Recommended
Polimeri Europa Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FF 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 45 show high toughness.Main Applications: Greenflex FF 45 is recommended for..
Thickness 30.0 - 150 microns
1.18 - 5.91 mil
Recommended
Polimeri Europa Greenflex® FF 55 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FF 55 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 55 show high flexibility.Main Applications: Greenflex FF 55 is recommended f..
Thickness 30.0 - 150 microns
1.18 - 5.91 mil
Recommended
Polimeri Europa Greenflex® FL 25 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FL 25 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FL 25 show good optical properties and excellent sealability.Main Applications: ..
Thickness 40.0 - 150 microns
1.57 - 5.91 mil
Recommended
Polimeri Europa Riblene® FC 39 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 39 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 39 is characterized by a high melt strength leading to a good bubble stability..
Thickness 40.0 - 150 microns
1.57 - 5.91 mil
Recommended
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability..
Thickness 40.0 - 150 microns
1.57 - 5.91 mil
Recommended
Polimeri Europa Riblene® FF 20 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 20 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FF 20 is characterized by a good melt strength leading to a good bubble stability..
Thickness 40.0 - 150 microns
1.57 - 5.91 mil
Recommended
Polimeri Europa Riblene® FF 22 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 22 is a high molecular weight low density polyethylene (LDPE), with added slip agent, suitable for blown film extrusion. Riblene FF 22 is characterized by a good melt strength leading to..
Thickness 40.0 - 150 microns
1.57 - 5.91 mil
Recommended
Polimeri Europa Riblene® FF 24 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 24 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 24 is characterized by a good melt s..
Thickness 40.0 - 150 microns
1.57 - 5.91 mil
Recommended
Polimeri Europa Riblene® FF 29 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 29 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 29 is characterized by a good melt strength leading to a good bubble stabilit..
Thickness 30.0 - 150 microns
1.18 - 5.91 mil
Recommended
Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit..
Thickness 30.0 - 150 microns
1.18 - 5.91 mil
Recommended
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a ..
Thickness 30.0 - 150 microns
1.18 - 5.91 mil
Recommended
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s..
Thickness 30.0 - 150 microns
1.18 - 5.91 mil
Recommended
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit..
Thickness 25.0 - 150 microns
0.984 - 5.91 mil
Recommended range for processing
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film
FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
Thickness 40.0 - 150 microns
1.57 - 5.91 mil
Indium Corp. NanoFoil® High Temperature Nickel and Aluminum Sacrificial Heat Source
As a sacrificial heat source in soldering and brazing applications, NanoFoil® is ideal for high-temperature applications. NanoFoil becomes a non-functional part of the solder or braze joint, eli..
Thickness 20.0 - 150 microns
0.787 - 5.91 mil
possible range, depending on extrusion conditions
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film
LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of..
Thickness 25.0 - 150 microns
0.984 - 5.91 mil
Average value: 54.3 microns Grade Count:24
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..
Thickness 8.00 - 150 microns
0.315 - 5.91 mil
Average value: 33.9 microns Grade Count:20
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum..
Thickness 25.0 - 150 microns
0.984 - 5.91 mil
possible range, depending on extrusion conditions
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film
LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene..