NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Octene, Film
Manufacturer NOVA Chemicals
Trade Name Surpass®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chemicals' polyethylene resins are biologically and chemically inert.Features: Good stiffness, Easy processability, Very good toughness and strength, Excellent seal properties, Low gelAdditives: Process stabilizer, Antiblock at 3400 ppm, Polymer process aidApplications: Heavy duty shipping sacks requiring very good toughness and high stiffness, Industrial packaging, Industrial liners, Lamination filmFilm properties are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D 792
Thickness 25.0 microns
0.984 mil
As tested for properties on this data sheet
25.0 - 150 microns
0.984 - 5.91 mil
Recommended range for processing
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.00 MPa
1310 psi
ASTM D 882
Film Tensile Strength at Yield, TD 10.0 MPa
1450 psi
ASTM D 882
Film Elongation at Break, MD 520 %
520 %
ASTM D 882
Film Elongation at Break, TD 700 %
700 %
ASTM D 882
Elmendorf Tear Strength MD 290 g
290 g
ASTM D 1922
Elmendorf Tear Strength TD 490 g
490 g
ASTM D 1922
Elmendorf Tear Strength, MD 11.6 g/micron
295 g/mil
ASTM D 1922
Elmendorf Tear Strength, TD 19.6 g/micron
498 g/mil
ASTM D 1922
Dart Drop 20.5 g/micron
521 g/mil
ASTM D 1709/A
Dart Drop Test 512 g
1.13 lb
F50; ASTM D 1709/A
Film Tensile Strength at Break, MD 50.0 MPa
7250 psi
ASTM D 882
Film Tensile Strength at Break, TD 42.0 MPa
6090 psi
ASTM D 882
1% Secant Modulus, MD 174 MPa
25200 psi
ASTM D 882
1% Secant Modulus, TD 188 MPa
27300 psi
ASTM D 882
Optical Properties Metric English Comments
Haze 21 %
21 %
ASTM D 1003
Gloss 33 %
33 %
At 45°; ASTM D 2457
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F
Recommended
Die Opening 0.0889 - 0.203 cm
0.0350 - 0.0800 in
Recommended range
Descriptive Properties Value Comments
Low Friction Puncture 53 (J/mm)
NOVA Chemicals test method