Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 16 g/10 min @Load 21.6 kg, Temperature 190 °C |
16 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
SABIC F01552 High Density Polyethylene for Blown Film Product Description: F01552 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® INP572 ABS High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® INP572 ABS+SAN High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® MG37CR ABS (Asia Pacific) High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® S702S ABS (Europe-Africa-Middle East) CYCOLAC S702S is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries. Cycolac S702S is anti-dust equiped.. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 260 °C |
16 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 260 °C |
16 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 260 °C |
16 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 260 °C |
16 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 260 °C |
16 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS2S PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 260 °C |
16 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East) XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 200 °C |
16 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G2780C Thermoplastic Elastomer (TPE) Dynaflex™ G2780C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmold A.. |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 16 - 30 g/10 min @Load 5.00 kg, Temperature 230 °C |
16 - 30 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Melt Flow | 16 - 56 g/10 min @Load 21.6 kg, Temperature 190 °C |
16 - 56 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 360 °C |
16 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 360 °C |
16 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Melt Flow | 16 g/10 min @Load 6.60 kg, Temperature 337 °C |
16 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1110FV PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data was supplied by SABIC-I.. |
|||
Melt Flow | 16 g/10 min @Load 6.60 kg, Temperature 337 °C |
16 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1110R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 16 g/10 min @Load 6.60 kg, Temperature 337 °C |
16 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 16 g/10 min @Load 6.60 kg, Temperature 337 °C |
16 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1110V PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 360 °C |
16 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 220 °C |
16 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Melt Flow | 16 - 30 g/10 min @Load 5.00 kg, Temperature 230 °C |
16 - 30 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 200 °C |
16 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 200 °C |
16 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 260 °C |
16 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® APC100 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites, Inc. |