Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 120 cm³/g | 120 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Viscosity Test | 120 cm³/g | 120 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Viscosity Test | 120 cm³/g | 120 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |
|||
Viscosity Test | 120 cm³/g | 120 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66
(Unverified Data**) 43% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G43HSLA BK099 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Viscosity Test | 120 cm³/g | 120 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® HTN FR52G30BL NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Viscosity Test | 120 cm³/g | 120 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Viscosity Test | 120 cm³/g | 120 cm³/g | Viscosity Number |
Arkema Group Lacovyl® PA 1384 Vinyl Copolymer LACOVYL PA 1384 is a vinyl chloride and vinyl acetate (4 %) copolymer manufactured by microsuspension polymerization process for the preparation of plastisols and fuses at comparatively low temperat.. |
|||
Viscosity Test | 120 cm³/g | 120 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |