Material Notes:
Georgia Gulf 5006 White is a rigid PVC pellet compound designed for extrusion of rigid PVC house siding, window profiles and various contours where maximum weather resistance is required. Georgia Gulf 5006 White is widely used for window profiles and house siding. Twin screw extruded sheet and kick panels are also produced. USDA approval allows 5006 to be used for walk-in cooler walls, refrigerated truck panels and associated profiles. Single or twin screw machines may be used to convert Georgia Gulf 5006 White. It has been designed with excellent impact at ambient temperatures. The high flexural and tensile strength makes it highly suitable for structural installation. The extrusion flow characteristics are excellent, and complicated panel profiles are easily filled out, requiring a minimum of pull-down.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D-785
Hardness, Shore D 82
82
ASTM D-2240
Tensile Strength, Yield 49.0 MPa
7100 psi
ASTM D-638
Tensile Modulus 3.10 GPa
450 ksi
ASTM D-638
Flexural Strength 84.1 MPa
12200 psi
ASTM D-790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D-790
Izod Impact, Notched 0.801 J/cm

@Thickness 6.35 mm
1.50 ft-lb/in

@Thickness 0.250 in
ASTM D-256
1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 137 kJ/m²
65.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C
156 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F
Descriptive Properties Value Comments
Cell Classification 13464
ASTM D-1784