Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D5420 |
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D5420 |
RheTech Products FT4700-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP3-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, High Flow Polycarbonate, FDA-compliant Feedstocks, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources NY66-IM2 Impact Modified Nylon 66 Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are .. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources NY6-IM1-[color]-H Nylon 6, Impact Modified, Heat Stabilized Nylon 6, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP1-TFE10 Polycarbonate, 10% PTFE, Wear Resistant, Low Flow Polycarbonate, 10% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | Average value: 36.2 J Grade Count:3 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Gardner Impact | 36.2 J @Temperature -30.0 °C |
26.7 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
DuPont Bexloy® AXW507NC010 Modified Ionomer Resin
(discontinued **) A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | ASTM D5420 |
Flint Hills P5C4K-089 Random Copolymer Polypropylene Features: Good clarity. Product does not contain animal derived components. Phthalate-freeApplications: Cast FilmInformation provided by Flint Hills Resources. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | ASTM D5420 |
Flint Hills P5G2N-093 Random Copolymer Polypropylene Features: Nucleated. Product does not contain animal derived components.Applications: Compression molding, Caps and ClosuresInformation provided by Flint Hills Resources. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | face |
Master Bond UV15SP-1 Low Viscosity, UV Curable System Description: Master Bond UV15SP-1 is a new one component, high strength UV curable epoxy resin based polymer system for bonding, sealing, & coating with high performance properties. It is a 100% rea.. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Diamond Polymers NPP 808 C2 Polycarbonate Alloy, Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Diamond Polymers NPP 808 C2 TDS Polycarbonate Alloy, Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | 36.2 J @Temperature 23.0 °C |
26.7 ft-lb @Temperature 73.4 °F |
1/2" R Tup125 mil |
Axiall SP-6340 Rigid PVC, Molding Georgia Gulf SP-6340 is a rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum burst strength is required. Georgia Gulf 6340 is ideally suited .. |
|||
Gardner Impact | 36.2 J @Temperature 23.0 °C |
26.7 ft-lb @Temperature 73.4 °F |
1/2" R Tup, 123 mil |
Axiall SP-7221 Rigid PVC, Molding Georgia Gulf SP-7221 is a high impact rigid vinyl compound designed for water distribution systems. The product is NSF listed under Standard 14.Information provided by Georgia GulfGeorgia Gulf beca.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | Average value: 36.2 J Grade Count:3 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | Average value: 36.2 J Grade Count:4 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |