Polymer Property : Ball Indentation Hardness = 95.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 95.0 MPa
13800 psi
ISO 2039-1
Nilit FRIANYL A63 HS28 Nylon 6.6 for injection molding
Nylon 6.6 for injection molding, maximum cold and dry impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 95.0 MPa
13800 psi
ISO 2039-1
Nilit FRIANYL A63 HS-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced
Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 95.0 MPa
13800 psi
ISO 2039-1
Nilit FRIANYL B63 HS-GV 5 Nylon 6 for injection molding, 5% glass fiber reinforced
Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 95.0 MPa
13800 psi
ISO 2039-1
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data)
Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro..
Ball Indentation Hardness 95.0 - 115 MPa
13800 - 16700 psi
Average value: 104 MPa Grade Count:13
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Ball Indentation Hardness 95.0 - 120 MPa
13800 - 17400 psi
Average value: 109 MPa Grade Count:7
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Ball Indentation Hardness 95.0 - 115 MPa
13800 - 16700 psi
Average value: 107 MPa Grade Count:3
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Ball Indentation Hardness 95.0 MPa
13800 psi
ISO 2039-1
Styrolution Novodur® E309 ABS
Novodur E309 is a extrusion grade especially designed for furniture profilesInformation provided by Styrolution
Ball Indentation Hardness 95.0 MPa
13800 psi
ISO 2039-1
Styrolution Novodur® H701 ABS
Novodur H701 is an injection molding grade of ABS with heat resistance and high impact strength.Information provided by Styrolution
Ball Indentation Hardness 95.0 MPa
13800 psi
ISO 2039-1
Styrolution Novodur® P2M-AT ABS Pellets
Novodur® P2M-AT has high impact strength, high gloss, and contains antistatic additive. It is used for the production of molded plastic articles.
Ball Indentation Hardness 95.0 MPa
13800 psi
ISO 2039-1
Styrolution Terblend® N NG-02 UV ABS / PA, 8% Glass filled
Terblend N NG-02 UV is an 8% glass fiber reinforced (UV stabilized) ABS/PA blend with enhanced dimensional stability and rigidity.High dimensional stabilityEnhanced rigidityEnhanced softening temper..
Ball Indentation Hardness 95.0 MPa
13800 psi
dry; ISO 2039-1
EMS-Grivory Grivory® AZ 3 PA66
Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures..
Ball Indentation Hardness 95.0 MPa
13800 psi
dry; ISO 2039-1
EMS-Grivory Grivory® AZ 3/2 PA66
Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE..
Ball Indentation Hardness 95.0 MPa
13800 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BFZ 3 PA6
Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril..
Ball Indentation Hardness 95.0 MPa
13800 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BZ 3 PA6
Information provided by EMS Grivory
Ball Indentation Hardness 95.0 MPa
13800 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® LV-2A NZ PA12-GF20
Product description: Grilamid LV-2A NZ is a high viscosity polyamide 12 with 20% glass fibers and improved hydrolysis resistance compared to standard polyamide 12 materials. Grilamid LV-2A NZ has a ..
Ball Indentation Hardness 95.0 MPa
13800 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSGZ-30 PA666-GF30
Product description: Grilon TSGZ-30 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSGZ-30 has the following important p..
Ball Indentation Hardness 95.0 MPa

@Time 30.0 sec
13800 psi

@Time 0.00833 hour
DIN 53 456
Hippe PA 12 Nylon 12
Maintenance-free bearing and gear components under water, insulated components, seals, gear wheels. Parts for pumps and household units. Application in the electrical sector - less water absorptio..
Ball Indentation Hardness 95.0 MPa
13800 psi
H358/30; ISO 2039-1
Chi Mei Polylac® PA-758R ABS - Transparent
Transparent, Chemical Resistant
Ball Indentation Hardness 95.0 MPa

@Load 36.5 kg,
Time 30.0 sec
13800 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Luran® S KR 2861/1 C Colored ASA+PC
Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh..
Ball Indentation Hardness 95.0 - 155 MPa
13800 - 22500 psi
Average value: 127 MPa Grade Count:3
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..