Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.420 J/cm² @Temperature -40.0 °C |
2.00 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 HH-TFGV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.420 J/cm² | 2.00 ft-lb/in² | ISO 179/1eA |
Radici Raditer® BN100 Polybutylene Terephthalate PBT General PurposeInformation provided by Radici group. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature 23.0 °C |
2.00 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179/1eA |
PolyOne Bergadur™ PB400 G10 H UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature -40.0 °C |
2.00 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 HH-SG-GV 2020 Nylon 6.6 for injection molding, 20% mineral filled, 20% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature 23.0 °C |
2.00 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Charpy Impact, Notched | 0.420 - 1.06 J/cm² @Temperature -30.0 - -30.0 °C |
2.00 - 5.04 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.712 J/cm² Grade Count:5 |
Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Charpy Impact, Notched | 0.420 - 0.460 J/cm² @Temperature -30.0 - -30.0 °C |
2.00 - 2.19 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.440 J/cm² Grade Count:2 |
Overview of materials for Nylon 11 with Graphite Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with Graphite Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact, Notched | 0.420 - 0.560 J/cm² | 2.00 - 2.67 ft-lb/in² | Average value: 0.490 J/cm² Grade Count:6 |
Overview of materials for Nylon 12, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature -20.0 °C |
2.00 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
IRPC Polimaxx Polene 2100N Polypropylene Block Copolymer CHARACTERISTICS: MEDIUM FLOW, HIGH STIFFNESSAPPLICATIONS: INJECTION MOLDING FOR HOUSEWARES, ELECTRICAL PARTS, AUTOPARTS |
|||
Charpy Impact, Notched | 0.420 J/cm² | 2.00 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® CRN7000 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50% DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.420 J/cm² | 2.00 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® HN7315 Polybutylene Terephthalate (PBT), Low warpage, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature -30.0 °C |
2.00 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastar 6763 PETG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature 23.0 °C |
2.00 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature -30.0 °C |
2.00 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Conditioned) Designation ISO 1874-PA12,EHLS,22-010,CD10Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Very low friction coefficient. No.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature -30.0 °C |
2.00 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Conditioned) Designation ISO 1874-PA12,MHLS,14-010,CD05Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature -30.0 °C |
2.00 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Dry) Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good .. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature -30.0 °C |
2.00 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BESN P40 W5 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EFHL,22-003Flexible grade for tubes extrusion. Available color: milky white. Light and heat stabilized. Flame retardant agent.Fire-resistant. Flexibility. High impact str.. |
|||
Charpy Impact, Notched | 0.420 J/cm² | 2.00 ft-lb/in² | |
Arkema Group Rilsan® MB 3000 Nylon 11, Sheathing Grade (Dry) Designation ISO 1874-PA11,MF,12-010Polyvalent rigid grade for injection molding and sheathing of cables. Available color: natural. Flame retardant agent, halogen free. Fire-resistant. Easy to be pro.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Thickness 2.00 mm, Temperature 20.0 °C |
2.00 ft-lb/in² @Thickness 0.0787 in, Temperature 68.0 °F |
ASTM D256 |
Mitsui TPX® MX002 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Thickness 2.00 mm, Temperature 20.0 °C |
2.00 ft-lb/in² @Thickness 0.0787 in, Temperature 68.0 °F |
ASTM D256 |
Mitsui TPX® MX004 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Thickness 2.00 mm, Temperature 20.0 °C |
2.00 ft-lb/in² @Thickness 0.0787 in, Temperature 68.0 °F |
ASTM D256 |
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Thickness 2.00 mm, Temperature 20.0 °C |
2.00 ft-lb/in² @Thickness 0.0787 in, Temperature 68.0 °F |
ASTM D256 |
Mitsui TPX® RT18 XB Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature -30.0 °C |
2.00 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |