Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
Pasargad Polymer Peyvand Pasamid 3P-H2130B1 Nylon 66, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
Celanese VECTRA E130i LCP, 30% Glass Reinforced
(Unverified Data**) High temperature capability, easiest flow. Suitable where very thin walls are required. Used for broad range of SMT applications, with minimal dimensional change. 30% glass filled.30% glass fiber, e.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | |
Ineos ABS Lustran® 348 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Europe-Africa-Middle East) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
Teijin Multilon TN-7100F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. High stiffness and flowability realize the thin wall of large-scale business machine chassis.Information provided by Tei.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO Data, Low Temp |
Styron Pulse® 1350 ABS + Polycarbonate PULSE® 1350 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
Polyram Polytron P50B07 Polypropylene, 50% Long Glass Fiber, UV Stabilized A chemically coupled 50% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65 Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW200F8 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | DIN 53453, Ductile break |
DSM Fibre Intermediates Nyrim® 2000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179-2 |
Denka MALECCA K-090 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT) Unreinforced Renewably Sourced Polytrimethylene Terephthalate with Excellent Impact Resistance Sorona MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -20.0 °C |
10.5 ft-lb/in² @Temperature -4.00 °F |
After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® LE 6000 Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -20.0 °C |
10.5 ft-lb/in² @Temperature -4.00 °F |
After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® LE60 THM Polyamide Alloy Polyamide Alloy, Semi-Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Orgalloy® LT 4060 Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrates a good balance of properties eg, high flexibility (200 MPa), good.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | |
BASF Luranyl® KR 2404 Polyphenylene Ether + Styrene-Butadiene Blend Base grade with high heat deformation resistance and a balanced combination of stiffness and toughness. Uses include: steering-wheel covers and heater controls.Data was collected by ISO methods and.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
Celanese Celstran® PPS-GF40-01 AD3002 Black PPS, 40% Glass Reinforced 40% long strand fiber glass reinforced polyphenylene sulfideInformation provided by Celanese |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Celanese RITEFLEX 663 TPC, Unfilled Riteflex 663 is a nominal 63 Shore D thermoplastic polyester elastomer with medium modulus.Information provided by Celanese |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
Celanese VECTRA E130i LCP, 30% Glass Reinforced High temperature capability, easiest flow. Suitable where very thin walls are required. Used for broad range of SMT applications, with minimal dimensional change. 30% glass filled.Information provid.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
BASF Ultramid® TG7S BK-102 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified nylon 6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushi.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® RS 6030 Polyamide 6 Alloy 30% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC STAMAX 40YM243 PP SABIC® STAMAX 40YM243 is a 40% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS .. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Celanese Celstran® PP-GF30-0403 P10/10 PP, 30% Glass Reinforced Material code according to ISO 1043-1: PPInformation provided by Celanese |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |