Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica PE 500 - Polyethylene 500 Polyethylene with a molecular weight of ± 500,000. PE 500 is more rigid than the high molecular weight polyethylene and it is therefore more suitable for mechanical applications. The friction coeff.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO.179 DN.53453 |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500 PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Asia Pacific) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific) Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ADX1016R PC (Europe-Africa-Middle East) Lexan Copolymer resin with improved chemical resistance, available only in limited colors. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179/1eA |
Pasargad Polymer Peyvand Pasalac 3P-H9000B ABS/PC Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Asia Pacific) Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Asia Pacific) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® PK2870 PC (Asia Pacific) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® PK2870 PC (Europe-Africa-Middle East) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Asia Pacific) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179 |
Nilit Nilamid A3 H ZC High Impact PA66 Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | DIN 53453 |
Nilit FRIANYL C73 HS28 Nylon 6.6/6 for injection molding Nylon 6.6/6 for injection molding, medium viscosity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179 |
GEHR Plastics PP Polypropylene Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle... |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 0500 Unsaturated Polyester UP SMC 0500 is a special SMC with reduced density. The glass level has been selected to combine good moulding with good strength and stiffness properties. Even without a specific fire retardant the fir.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X5100 PC+PBT (Europe-Africa-Middle East) XENOY X5100 is a semi-crystalline, impact modified PC-PBT blend with excellent flow. (PC+PBT-I). |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179/1eA |
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo.. |
|||
Charpy Impact, Notched | 5.00 - 10.0 J/cm² | 23.8 - 47.6 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Covestro Makroblend® KU 2-7915 Polycarbonate + PBT, Impact Grade ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradeexcellent toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® XE 4188 nat PA612 Product description: Grilamid XE 4188 natural is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 natural are: High viscosi.. |
|||
Charpy Impact, Notched | >= 5.00 J/cm² | >= 23.8 ft-lb/in² | Determined with double-notched specimens; ISO 11542-2 |
Braskem Idealis 500 High Molecular Weight Polyethylene Powder Braskem Idealis 500 is the only High Molecular Weight Polyethylene resin in powder form specially designed for the compression molding process; Applications range from food handling cutting boards a.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® B3S HP PA6 (Conditioned) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |