Material Notes:
Zellamid® 1100 is the registered trademark for Zell-Metall’s cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers excellent machineability and chemical resistance. Standard color is ivory. Black and blue are available upon request.Zellamid® 1100 is ideally suited for heavy duty plastic components and offers many advantages in comparison with steel: corrosion resistance, low weight, and low wear - e.g. for crane sheaves or carriage wheels for ropeways which are produced as finished parts by spin casting.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Dry Density
Moisture Absorption at Equilibrium 2.5 - 3.0 %
2.5 - 3.0 %
Saturation at 50% RH
Water Absorption at Saturation 6.0 - 7.0 %
6.0 - 7.0 %
23°C
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 80
78 - 80
DIN 53505
Tensile Strength at Break 68.0 - 70.0 MPa
9860 - 10200 psi
DIN 53455
Elongation at Break 40 - 80 %
40 - 80 %
DIN 53455
Tensile Modulus 2.50 GPa
363 ksi
DIN 53457
0.400 GPa

@Temperature 100 °C
58.0 ksi

@Temperature 212 °F
DIN 53457
Charpy Impact, Notched 5.00 - 10.0 J/cm²
23.8 - 47.6 ft-lb/in²
DIN 53453
Coefficient of Friction 0.050 - 0.10
0.050 - 0.10
to steel, added lubrication
0.30 - 0.35
0.30 - 0.35
to steel, no lubrication; ISO/DTR 7147
Tensile Creep Modulus, 1000 hours <= 500 MPa
<= 72500 psi
DIN 53444
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 1.67 J/g-°C
0.399 BTU/lb-°F
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 220 °C
428 °F
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long time operation
120 - 140 °C
248 - 284 °F
medium time operation
160 °C
320 °F
a few hours operation
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+12 - 5.00e+12 ohm-cm
3.00e+12 - 5.00e+12 ohm-cm
DIN 53482
Surface Resistance 1.00e+10 - 3.00e+10 ohm
1.00e+10 - 3.00e+10 ohm
DIN 53482
Dielectric Constant 12

@Frequency 1e+6 Hz
12

@Frequency 1e+6 Hz
DIN 53483
Dielectric Strength 15.0 - 20.0 kV/mm
381 - 508 kV/in
DIN 53481
Dissipation Factor 0.15

@Frequency 1e+6 Hz
0.15

@Frequency 1e+6 Hz
DIN 53483
Comparative Tracking Index 600 V
600 V
KV Method; DIN 53480
Descriptive Properties Value Comments
Time yield limit up to 8.5