Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.500 - 3.00 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 14.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.25 J/cm² Grade Count:29
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Charpy Impact, Notched 0.500 - 3.00 J/cm²
2.38 - 14.3 ft-lb/in²
Average value: 1.62 J/cm² Grade Count:19
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Charpy Impact, Notched 1.50 - 3.00 J/cm²

@Temperature -30.0 - 30.0 °C
7.14 - 14.3 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 2.29 J/cm² Grade Count:7
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Charpy Impact, Notched 0.400 - 3.00 J/cm²
1.90 - 14.3 ft-lb/in²
Average value: 1.21 J/cm² Grade Count:30
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Charpy Impact, Notched 3.00 - 3.00 J/cm²

@Temperature -20.0 - -20.0 °C
14.3 - 14.3 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 3.00 J/cm² Grade Count:1
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Charpy Impact, Notched 0.300 - 3.00 J/cm²

@Temperature -30.0 - -30.0 °C
1.43 - 14.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.10 J/cm² Grade Count:24
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Charpy Impact, Notched 0.300 - 3.00 J/cm²
1.43 - 14.3 ft-lb/in²
Average value: 1.25 J/cm² Grade Count:71
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Charpy Impact, Notched 0.600 - 3.00 J/cm²
2.86 - 14.3 ft-lb/in²
Average value: 1.44 J/cm² Grade Count:13
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Charpy Impact, Notched 2.50 - 3.00 J/cm²
11.9 - 14.3 ft-lb/in²
DIN 53453
Zell-Metall Engineering Plastics Zellamid 1100
Zellamid® 1100 is the registered trademark for Zell-Metall’s cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers ..
Charpy Impact, Notched 1.80 - 3.00 J/cm²
8.57 - 14.3 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound
UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot..
Charpy Impact, Notched 1.80 - 3.00 J/cm²
8.57 - 14.3 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR L 4305 Bulk Molding Compound
UL-licensed. Anchor wave-isolation.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prote..
Charpy Impact, Notched 0.400 - 3.00 J/cm²
1.90 - 14.3 ft-lb/in²
Average value: 1.42 J/cm² Grade Count:69
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Charpy Impact, Notched 0.600 - 3.00 J/cm²

@Temperature -30.0 - -30.0 °C
2.86 - 14.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.30 J/cm² Grade Count:10
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..