Izod Impact, Notched 0.240 - 0.290 J/cm
0.450 - 0.543 ft-lb/in
Average value: 0.259 J/cm Grade Count:15
Overview of materials for Phenolic, Novolac, Impact Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum ..
Izod Impact, Notched 0.210 - 0.290 J/cm
0.393 - 0.543 ft-lb/in
Average value: 0.250 J/cm Grade Count:4
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum ..
Izod Impact, Notched 0.230 - 0.290 J/cm
0.431 - 0.543 ft-lb/in
ASTM D256A
DSM Somos® GP Plus 14122
Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually ..
Izod Impact, Notched 0.170 - 0.290 J/cm
0.318 - 0.543 ft-lb/in
ASTM D256A
DSM Somos® ProtoCast™ AF 19122 Antimony-free Liquid Photopolymer
Product DescriptionDSM Somos® ProtoCast™ AF 19122 is an antimony-free liquid photopolymer specifically formulated for producing investment casting patterns.ApplicationsIdeal for use in foundry app..