Adell BJ-13 Nylon 6, 15% Glass Reinforced; High Impact

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Filled, Impact Grade
Manufacturer Adell Plastics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell BJ-13 Nylon 6, 15% Glass Reinforced; High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.80 %
0.80 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0075 cm/cm
0.0075 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 76
76
ASTM D785
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Ultimate 86.2 MPa
12500 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 108 MPa
15700 psi
ASTM D790
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Compressive Yield Strength 103 MPa
14900 psi
ASTM D695
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 199 °C
390 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Flammability, UL94 HB
HB