Ineos K44-08-123 HDPE Copolymer with Carbon Black

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Carbon Black Filled
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos K44-08-123 HDPE Copolymer with Carbon Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fortiflex® K44-08-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized by the Plastic Pipe Institute as having a PE 3408 rating. The natural version of this resin is available as Fortiflex® K44-08-122.2.3% Carbon Black Concentration
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ASTM D4883
Environmental Stress Crack Resistance >= 5000 hour
>= 5000 hour
Condition C; ASTM D 1693
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.810 GPa
117 ksi
2% Secant-Method 1; ASTM D790
Izod Impact, Notched 3.20 J/cm
5.99 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746