Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
With Flow; ISO 2577
0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 60.0 MPa
<= 8700 psi
ISO/R527
Elongation at Yield 6.0 %
6.0 %
ISO/R527
Flexural Strength <= 100 MPa
<= 14500 psi
ISO 178
Flexural Modulus 2.20 GPa

@Temperature 23.0 °C
319 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 3.00 J/cm²

@Temperature -20.0 °C
14.3 ft-lb/in²

@Temperature -4.00 °F
ISO 179
4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
120°C/h; ISO 75/1
Vicat Softening Point 140 °C

@Load 5.001 kg
284 °F

@Load 11.03 lb
50°C/h; ISO 306
145 °C

@Load 1.00 kg
293 °F

@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Glow Wire Test 850 °C

@Thickness 2.00 mm
1560 °F

@Thickness 0.0787 in
IEC 695-2-1