Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
North Wood Plastics PS with 20% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Izod Impact, Unnotched | 0.801 - 5340 J/cm | 1.50 - 10000 ft-lb/in | Average value: 6.47 J/cm Grade Count:296 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Izod Impact, Unnotched | 0.801 - 10.7 J/cm | 1.50 - 20.0 ft-lb/in | Average value: 3.62 J/cm Grade Count:22 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Unnotched | 0.801 J/cm - NB | 1.50 ft-lb/in - NB | Average value: 7.52 J/cm Grade Count:12 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Unnotched | 0.801 - 8.54 J/cm | 1.50 - 16.0 ft-lb/in | Average value: 5.11 J/cm Grade Count:44 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched | 0.800 - 1.20 J/cm @Temperature 23.0 °C |
1.50 - 2.25 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 265/D Rigid PVC, Extrusion Semi-rigid furniture border |
|||
Izod Impact, Unnotched | 0.800 - 1.20 J/cm @Temperature 23.0 °C |
1.50 - 2.25 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 210/K1 Rigid PVC, Antishock Extrusion Antishock profiles |
|||
Izod Impact, Unnotched | 0.800 - 1.20 J/cm @Temperature 23.0 °C |
1.50 - 2.25 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RST 0413 Rigid PVC, Extrusion Lead Free Transparent antishock profiles |
|||
Izod Impact, Unnotched | 0.800 J/cm | 1.50 ft-lb/in | |
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be.. |
|||
Izod Impact, Unnotched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
E-48/50 |
Industrial Laminates/Norplex MC320LE Cotton Fabric Description: Grade MC320LE is a fine weave bleached cotton phenolic composite that has excellent machining characteristics and low moisture absorption. Applications include marine applications, term.. |
|||
Izod Impact, Unnotched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Spartech Litho SP-2090 Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrafil® J-50/CF/10/TF/15 Polycarbonate, 10% Carbon Fiber Reinforced, 15% PTFE |
|||
Izod Impact, Unnotched | 0.801 - 1.33 J/cm | 1.50 - 2.50 ft-lb/in | ASTM D256 |
CPC - Vycom FLAMETEC™ KYTEC® PVDF Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e.. |
|||
Izod Impact, Unnotched | 0.800 - 1.20 J/cm @Temperature 23.0 °C |
1.50 - 2.25 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds ART 0665/S Rigid PVC, Atoxic for General Purpose Injection moulding and blow moulding bottles |
|||
Izod Impact, Unnotched | 0.800 - 1.20 J/cm @Temperature 23.0 °C |
1.50 - 2.25 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds R 211 Rigid PVC, Extrusion Shutters and shiny profiles |
|||
Izod Impact, Unnotched | 0.800 - 1.20 J/cm @Temperature 23.0 °C |
1.50 - 2.25 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds R 212/C Rigid PVC, Extrusion Shutters and shiny profiles |
|||
Izod Impact, Unnotched | 0.801 - 16.0 J/cm | 1.50 - 30.0 ft-lb/in | Average value: 7.99 J/cm Grade Count:66 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Unnotched | 0.801 - 5340 J/cm | 1.50 - 10000 ft-lb/in | Average value: 8.47 J/cm Grade Count:46 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |