Charpy Impact Unnotched 15.0 J/cm²

@Temperature -20.0 °C
71.4 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVASTER® B1 BT PBT, basic type
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -20.0 °C
71.4 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)  (Unverified Data**)
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper..
Charpy Impact Unnotched >= 15.0 J/cm²

@Temperature 23.0 °C
>= 71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1eU
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Lanxess Durethan® A 30 S 000000 Nylon 66
PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins
Charpy Impact Unnotched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Lanxess Durethan® A 30 S 000000 Nylon 66
PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins
Charpy Impact Unnotched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
d.a.m.; ISO 179-1eU
Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding
PA 66, non-reinforced, injection moldingInformation provided by LANXESS.
Charpy Impact Unnotched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
d.a.m.; ISO 179-1eU
Lanxess Durethan® B 30 S F30 000000 Nylon 6, Flame Retardant
PA 6, non-reinforced, injection molding, flame retardantInformation provided by LANXESS.
Charpy Impact Unnotched >= 15.0 J/cm²

@Temperature 23.0 °C
>= 71.4 ft-lb/in²

@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls
PA6, molding grade, micro glass balls, good heat-ageing resistance
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® B 1300 000000 PBT
PBT, non-reinforced, injection molding, extrusion
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® B 1305 000000 PBT
PBT, non-reinforced, injection molding
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® KU 1-7301 000000 PBT
PBT, non-reinforced, injection molding, food contact
Charpy Impact Unnotched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1eU
Ineos ABS Lustran® ABS E211 LNS013 Pellets (a-methylstyrene-SAN-modified), Extrusion Grade
Lustran® ABS E211 LNS013 is extrusion grade with high heat resistance. It is used for the production of molded plastic articles.
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Styrolution Luran® S 776 S Colored ASA
Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j..
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Styrolution Luran® S 776 S UV ASA
Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j..
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Styrolution Luran® S 796 M Colored ASA
Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Charpy Impact Unnotched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Styrolution Novodur® E211 ABS
Novodur E211 is a high heat extrusion grade and suitable for blow moldingInformation provided by Styrolution
Charpy Impact Unnotched <= 15.0 J/cm²

@Temperature 23.0 °C
<= 71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Polystyrol 454 C GR 2 PS
Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts..
Charpy Impact Unnotched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 179/1eU
SYNTHOS Krasten® 662E High Impact Polystyrene
High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of demanding visual appearance plates, technical parts, sheets and molded pa..
Charpy Impact Unnotched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled
Terblend N 3154 is an 8% mineral filled ABS/PA blend with good dimensional stability and enhanced rigidity.High dimensional stabilityEnhanced rigidityMineral filled (8%)Information provided by Styro..
Charpy Impact Unnotched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Borealis Daplen™ EG103AI Polypropylene Compound, Mineral Filled
Daplen™ EG103AI is a 15 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and high melt flow rate..
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
longitudinal; ISO 179/1eU
Bond Laminates TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate
Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is ae..
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® N2770 K POM
Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF
Charpy Impact Unnotched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® N2770 K POM
Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® W2320 003 PRO POM
Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF
Charpy Impact Unnotched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® W2320 003 PRO POM
Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® W2320 U03 POM
Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF
Charpy Impact Unnotched 15.0 J/cm²

@Temperature -30.0 °C
71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by..
Charpy Impact Unnotched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1eU
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.