Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched (ISO) = 21.4 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 23.0 - 45.0 kJ/m²
10.9 - 21.4 ft-lb/in²
Average value: 36.5 kJ/m² Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Izod Impact, Unnotched (ISO) 32.0 - 45.0 kJ/m²
15.2 - 21.4 ft-lb/in²
Average value: 40.7 kJ/m² Grade Count:3
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
Izod Impact, Unnotched (ISO) 20.0 - 45.0 kJ/m²
9.52 - 21.4 ft-lb/in²
Average value: 26.3 kJ/m² Grade Count:6
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Izod Impact, Unnotched (ISO) 40.0 - 45.0 kJ/m²

@Temperature -30.0 - -30.0 °C
19.0 - 21.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 41.3 kJ/m² Grade Count:4
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Izod Impact, Unnotched (ISO) 35.0 - 45.0 kJ/m²
16.7 - 21.4 ft-lb/in²
Average value: 38.3 kJ/m² Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Izod Impact, Unnotched (ISO) 15.0 - 45.0 kJ/m²
7.14 - 21.4 ft-lb/in²
Average value: 27.0 kJ/m² Grade Count:5
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Izod Impact, Unnotched (ISO) 25.0 - 45.0 kJ/m²

@Temperature -40.0 - -30.0 °C
11.9 - 21.4 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 34.4 kJ/m² Grade Count:8
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Izod Impact, Unnotched (ISO) 25.0 - 45.0 kJ/m²
11.9 - 21.4 ft-lb/in²
Average value: 33.3 kJ/m² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved