Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa KOBLEND PCA PD 935 G2 PC+ABS, 10% Glass Fiber
(discontinued **) Symbol according to ISO 1043/1/2: PC+ABS (GF) Injection moulding grade, reinforced with 10% glass fibres, high stiffness, very good dimensional stability. Vicat/B50 = 135°C Main application field.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 50.0 kJ/m² @Temperature -30.0 - -30.0 °C |
19.0 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 45.0 kJ/m² Grade Count:1 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | |
Idemitsu Kosan Xarec® WA 214 SPS, 40% Glass Filled |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® ECO PA GF30 909040 Nylon 6, 30% Glass Fiber PA 6 (mainly), 30% glass fibers, injection molding, contains at least 80% pre-consumer recycled material, properties may change considerably from lot to lotInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP LCL36E PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LCL36E is a compound based on Polyetheretherketone resin containing Carbon Fiber , PTFE. Added features include : Electrically Conductive, Internally Lubricated, Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp RFN16SXS PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN16SXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Euro.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp UCL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36AS is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.This data .. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2300 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2310 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 48.0 kJ/m² | 19.0 - 22.8 ft-lb/in² | Type 1; ISO 180 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East) VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DC004E PC (Europe-Africa-Middle East) LNP* Thermocomp* DC004E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP JF006 PES LNP* THERMOCOMP* JF006 is a compound based on Polyethersulfone resin containing 30% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp LC008 PEEK (Europe-Africa-Middle East) LNP* Thermocomp* LC008 is a compound based on Polyetheretherketone resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Xenoy® XD1607 PBT+PC (Europe-Africa-Middle East) 22% Glass filled PBT+PC with a designed balance between surface appearance and mechanical properties sufficient for automotive doorhandle requirements. Special suitable for gas assist mouldings .Thi.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO 180/1U |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide PF004EUC PA6, 20% Glass Filled, Injection Molded PF004EUC is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam RF0055E PA66/6, 25% Glass Filled, Injection Molded Starflam RF0055E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z250EM)Information provided by Polym.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR25 NL XA60 PA6.6, 25% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G10 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated, Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Europe-Africa-Middle East) LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 68.0 kJ/m² | 19.0 - 32.4 ft-lb/in² | Average value: 50.7 kJ/m² Grade Count:13 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |