Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² - NB | 30.9 ft-lb/in² - NB | Average value: 65.0 kJ/m² Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Izod Impact, Unnotched (ISO) | 65.0 - 95.0 kJ/m² | 30.9 - 45.2 ft-lb/in² | Average value: 82.2 kJ/m² Grade Count:7 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Asia Pacific) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP SFL36 PA12 (Europe-Africa-Middle East) LNP* LUBRICOMP* SFL36 is a compound based on PA 12 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | Type 1; ISO 180 |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | Type 1; ISO 180 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon FX99030 PE (Europe-Africa-Middle East) LNP * Stat-kon* FX99030 is a compound based on Polyethylene resin containing Carbon Powder. Added features include: Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-M.. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON WEF32ISP PBT (Europe-Africa-Middle East) LNP * Stat-kon* WEF32ISP is a compound based on Polybutylene Terephalate resin containing Glass Fiber and Carbon Fiber. Added features include High Impact, Heat Stabilized and Electrically Conduct.. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF004XXC PC (Europe-Africa-Middle East) Polycarbonate compound, countaining Glass Fiber |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF008ER PC (Europe-Africa-Middle East) LNP* Thermocomp* DF008ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp PF0069 PA 6 (Europe-Africa-Middle East) LNP* STARFLAM* PF0069 is a compound based on PA 6 resin containing Glass Fiber, Flame Retardant. Added features include; Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC006 is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF00AS PA 66 LNP THERMOCOMP* RF00AS is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP UF00AAS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF00AAS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA6 30V D31 PA6, Glass Filled, Injection Molding Star L PA6 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA6 30V D61 PA6, Glass Filled, Injection Molding Star L PA6 30V D61 is a PTFE/Silicone Oil Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen MX06023 PP, 20% Milled Glass Fiber Filled, Injection Molded Starpylen MX06023 is a 20% Milled Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam PF0069 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0069 is a Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G30 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | ASTM D256 |
BLUESTAR 403G-MG30 PBT, 30% Glass Filled Typical Applications: High GWIT, RTI, E/EInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | ISO 180 |
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Amodel® A-6135 NL Polyphthalamide (PPA), 35% Glass Fiber Reinforcement
(discontin Amodel A-6135 NL polyphthalamide (PPA), a 35% glass reinforced, high-glow, non-lubricated, hot-water moldable resin specially designed for laser welding. The black version is a laser absorber, and t.. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² - NB @Temperature -30.0 - -30.0 °C |
30.9 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Average value: 76.7 kJ/m² Grade Count:15 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Unnotched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | ISO 180/U |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |