Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 23.0 - 55.0 kJ/m² | 10.9 - 26.2 ft-lb/in² | Average value: 42.3 kJ/m² Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 55.0 kJ/m² @Temperature -30.0 - -30.0 °C |
19.0 - 26.2 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 47.5 kJ/m² Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 - 55.0 kJ/m² | 11.9 - 26.2 ft-lb/in² | Average value: 40.2 kJ/m² Grade Count:6 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 55.0 kJ/m² | 7.14 - 26.2 ft-lb/in² | Average value: 31.3 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 55.0 kJ/m² | 9.52 - 26.2 ft-lb/in² | Average value: 28.3 kJ/m² Grade Count:11 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 - 55.0 kJ/m² | 14.3 - 26.2 ft-lb/in² | Average value: 39.4 kJ/m² Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Izod Impact, Unnotched (ISO) | 28.0 - 55.0 kJ/m² | 13.3 - 26.2 ft-lb/in² | Average value: 42.2 kJ/m² Grade Count:9 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |
|||
Izod Impact, Unnotched (ISO) | 17.0 - 55.0 kJ/m² | 8.09 - 26.2 ft-lb/in² | Average value: 37.3 kJ/m² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |