Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 15.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 12.0 - 15.0 kJ/m²
5.71 - 7.14 ft-lb/in²
ASTM D256
Polikim EFALON® C-25 PTFE, 25% Glass Filled
C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings..
Izod Impact, Notched (ISO) 10.0 - 15.0 kJ/m²
4.76 - 7.14 ft-lb/in²
Average value: 12.2 kJ/m² Grade Count:6
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Izod Impact, Notched (ISO) 2.60 - 15.0 kJ/m²

@Temperature -20.0 - -20.0 °C
1.24 - 7.14 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 5.34 kJ/m² Grade Count:13
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Izod Impact, Notched (ISO) 2.60 - 15.0 kJ/m²
1.24 - 7.14 ft-lb/in²
Average value: 7.65 kJ/m² Grade Count:18
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Izod Impact, Notched (ISO) 11.0 - 15.0 kJ/m²

@Temperature -40.0 - -40.0 °C
5.23 - 7.14 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 12.8 kJ/m² Grade Count:3
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Izod Impact, Notched (ISO) 10.0 - 15.0 kJ/m²

@Temperature -40.0 - -30.0 °C
4.76 - 7.14 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 11.1 kJ/m² Grade Count:7
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched (ISO) 4.00 - 15.0 kJ/m²

@Temperature -40.0 - -40.0 °C
1.90 - 7.14 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 9.83 kJ/m² Grade Count:8
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched (ISO) 3.99 - 15.0 kJ/m²
1.90 - 7.14 ft-lb/in²
Average value: 8.00 kJ/m² Grade Count:7
Overview of materials for Nylon 66, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat..
Izod Impact, Notched (ISO) 5.00 - 15.0 kJ/m²
2.38 - 7.14 ft-lb/in²
Average value: 10.0 kJ/m² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Izod Impact, Notched (ISO) 7.00 - 15.0 kJ/m²
3.33 - 7.14 ft-lb/in²
Average value: 12.5 kJ/m² Grade Count:11
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and ..
Izod Impact, Notched (ISO) 15.0 - 15.0 kJ/m²

@Temperature -30.0 - -30.0 °C
7.14 - 7.14 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 15.0 kJ/m² Grade Count:1
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..
Copyright © lookpolymers.com All Rights Reserved