Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.00 - 5.00 kJ/m²

@Temperature -30.0 - -30.0 °C
1.43 - 2.38 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.33 kJ/m² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Izod Impact, Notched (ISO) 5.00 - 5.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.38 - 2.38 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.00 kJ/m² Grade Count:1
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Izod Impact, Notched (ISO) 4.00 - 5.00 kJ/m²

@Temperature -40.0 - -40.0 °C
1.90 - 2.38 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 4.33 kJ/m² Grade Count:3
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched (ISO) 3.00 - 5.00 kJ/m²
1.43 - 2.38 ft-lb/in²
Average value: 4.22 kJ/m² Grade Count:9
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Izod Impact, Notched (ISO) 5.00 - 5.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.38 - 2.38 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.00 kJ/m² Grade Count:1
Overview of materials for Nylon 66, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Notched (ISO) 3.00 - 5.00 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 2.38 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.25 kJ/m² Grade Count:6
Overview of materials for Nylon 66, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat..
Izod Impact, Notched (ISO) 4.00 - 5.00 kJ/m²

@Temperature -30.0 - -30.0 °C
1.90 - 2.38 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.50 kJ/m² Grade Count:2
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched (ISO) 5.00 - 5.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.38 - 2.38 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.00 kJ/m² Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Izod Impact, Notched (ISO) 5.00 - 5.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.38 - 2.38 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.00 kJ/m² Grade Count:1
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..