Polymer Property : Izod Impact, Notched (ISO) = 20.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.00 - 20.0 kJ/m²
0.952 - 9.52 ft-lb/in²
Average value: 8.39 kJ/m² Grade Count:45
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched (ISO) 2.00 - 20.0 kJ/m²
0.952 - 9.52 ft-lb/in²
Average value: 13.8 kJ/m² Grade Count:12
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Izod Impact, Notched (ISO) 8.00 - 20.0 kJ/m²

@Temperature -40.0 - -40.0 °C
3.81 - 9.52 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 11.5 kJ/m² Grade Count:4
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Izod Impact, Notched (ISO) 8.00 - 20.0 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 9.52 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 12.6 kJ/m² Grade Count:4
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Izod Impact, Notched (ISO) 20.0 - 20.0 kJ/m²

@Temperature -40.0 - -40.0 °C
9.52 - 9.52 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 20.0 kJ/m² Grade Count:1
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Izod Impact, Notched (ISO) 11.0 - 20.0 kJ/m²

@Temperature -40.0 - -20.0 °C
5.23 - 9.52 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 14.6 kJ/m² Grade Count:17
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Izod Impact, Notched (ISO) 3.00 - 20.0 kJ/m²
1.43 - 9.52 ft-lb/in²
Average value: 8.40 kJ/m² Grade Count:37
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Izod Impact, Notched (ISO) 9.70 - 20.0 kJ/m²
4.62 - 9.52 ft-lb/in²
Average value: 15.6 kJ/m² Grade Count:7
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched (ISO) 15.0 - 20.0 kJ/m²
7.14 - 9.52 ft-lb/in²
ISO 180
Tisan TISAKRIL® UNR ABS
TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens..
Izod Impact, Notched (ISO) 10.0 - 20.0 kJ/m²
4.76 - 9.52 ft-lb/in²
Average value: 16.6 kJ/m² Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Izod Impact, Notched (ISO) 3.00 - 20.0 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 9.52 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 10.0 kJ/m² Grade Count:19
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Izod Impact, Notched (ISO) 5.00 - 20.0 kJ/m²
2.38 - 9.52 ft-lb/in²
Average value: 9.75 kJ/m² Grade Count:4
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..