Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y822-BP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness.Applications: Industrial packaging, high strength liners.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Surpass® FPs317-A Octene sLLDPE Film Resin Features: Exceptional puncture resistanceVery good tear propertiesLow gel levelExcellent optical properties Excellent elongation characteristics Easy to process, no drying required Applications: Cas.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend The Trilene TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring .. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ISO 527-3 |
Polimeri Europa Clearflex® CL B0 Very Low Density Polyethylene Clearflex CL B0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has a high stretchability and a good cling effect.Main Applications: C.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene CopolymerCharacteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applicationsApplications:Bakery Films, Coextr.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 76 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin
(discontinued **) Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplicat.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
ExxonMobil Escorene® LD 767.MJ Blown Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin PF-0218-B complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin PF-0218-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness, suitable for narrow die gaps.Applications: Heavy duty sacks, high strength packaging.Data provided by the manufac.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
Petroquimica Triunfo Trilene® TS 8058 LLDPE-C6 and LDPE Blend The Trilene TS 8058 product is a blend with a high ratio of linear low-density polyethylene - hexene comonomer (LLDPE-C6) with low-density polyethylene (LDPE) excellent mechanical resistance, along .. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | |
UBE 1022FDX23 Nylon 6 Homopolymer Film Specialties: High slip typeProcessing: Water cooling processTypical applications: small pouch & generalInformation provided by UBE. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ISO 527-3 |
Borealis FG5199 Linear Low Density Polyethylene FG5199 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-Fog and cling additives. The grade is developed for blown cling film. Film made from FG5199 is suit.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | 50 µm (2 mil) film; ASTM D882 |
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown 12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ISO 527-3 |
Total EVA 1005 VN 2 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 2 is made by a high pressure tubular process. Grade for transparent and resistant films. Contains an antioxidant.Application examples: Stretch, coextrusion, frozen food, agriculture fi.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | |
Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade DOWLEX® 2077 Polyethylene resin is a fully formulated linear low density polyethylene resin designed for use in food packaging applications. This blown film resin is designed to run on narrow die-g.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM-D882 |
Braskem TN2006 EVA General Film Copolymer TN2006 is an Ethylene-Vinyl Acetate (EVA) copolymer with good mechanical properties, high flexibility and toughness even with low temperature, and excellent optical and heat sealability properties. .. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
Huntsman Rexell® V8402 Cast Film Extrusion LLDPE
(discontinued **) Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent mechanical strength, low sealing temperature, and good flex crack resistanceApplications: Sealing layer in.. |
|||
Film Tensile Strength at Break, MD | 32.0 - 379 MPa | 4640 - 55000 psi | Average value: 184 MPa Grade Count:35 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati.. |
|||
Film Tensile Strength at Break, MD | 32.0 MPa | 4640 psi | ASTM D882 |
Chevron Phillips 6335B LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, Medium Slip Version of 6335Characteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applications, Lo.. |