Tensile Strength, Yield 29.0 - 68.9 MPa
4210 - 10000 psi
Average value: 32.2 MPa Grade Count:17
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..
Tensile Strength, Yield 32.0 - 68.9 MPa
4640 - 10000 psi
Average value: 45.3 MPa Grade Count:39
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..