Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 131 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 - 131 MPa
16000 - 19000 psi
Average value: 122 MPa Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Tensile Strength, Yield 75.8 - 131 MPa
11000 - 19000 psi
Average value: 116 MPa Grade Count:40
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Tensile Strength, Yield 50.0 - 131 MPa
7250 - 19000 psi
Average value: 87.4 MPa Grade Count:27
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Tensile Strength, Yield 55.2 - 131 MPa
8000 - 19000 psi
0.2% offset
Eagle Brass 230 Red Brass, Annealed
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Tensile Strength, Yield 82.7 - 131 MPa
12000 - 19000 psi
Average value: 114 MPa Grade Count:5
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Tensile Strength, Yield 131 - 131 MPa

@Temperature 93.3 - 93.3 °C
19000 - 19000 psi

@Temperature 200 - 200 °F
Average value: 131 MPa Grade Count:1
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Copyright © lookpolymers.com All Rights Reserved