Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.65 GPa | 239 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PQ 82 N 003/1M Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Tensile Modulus | 1.65 GPa @Temperature 23.9 °C |
240 ksi @Temperature 75.0 °F |
0° Direction, Dry; 325°F Autoclave; ASTM D638 |
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Commercial Silica Fabric Reinforced Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | |
Radici Radilon® A HSX (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | |
Radici Radilon® S USX200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | |
Radici Radilon® S USZ200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ASTM D638 |
PolyOne Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | |
Saint-Gobain Rulon® E Grade Bearing/Seal PTFE
(discontinued **) Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and .. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | |
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ASTM Test |
Styrolution Luran® S 776 SE ASA Luran S 776 SE is a general purpose extrusion ASA grade with good toughness and strength, used for sheet and profile extrusions.Information provided by STYROLUTION, which is a joint venture between .. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ISO 527-1/-2 |
Styrolution Polystyrol 485 I GR 2 PS Description: Polystyrol 485 I GR2 is a high-impact grade of polystyrene for extruded sheets with a matt surface.Applications: Sheet, semi finished goods, fat resistant food packaging.Information pro.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
ScanTube ECTFE Tubing Information provided by ScanTube, Inc. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1mm/min; ISO 527-2 |
Borealis BJ356MO Polypropylene Copolymer BJ356MO is a heterophasic copolymer. This grade provides very high melt flow rate, very high stiffness and medium impact strength. and is designed for high-speed injection molding and contains nucle.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ASTM D638 |
Westlake Plastics HIPS High Impact Polystyrene, Compression Molded Compression molded HIPS is a low cost plastic material that is easily machined and fabricated. It is frequently used for preproduction prototyping. HIPS is a FDA compliant use in food processing a.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ISO 527-2 |
Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | Tested using a 50 mil. Sheet; ASTM D638 |
Chevron Phillips EB6755 Rubber Modified Polystyrene DescriptionChevron EB6755 is an extrusion grade, high impact polystyrene developed for use in packaging applications. It is designed for exceptional environmental stress-crack resistance and practi.. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Ensinger Tecatron® XP-79 Compression Molded PPS Compound, 70% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ISO527-2/1 |
ExxonMobil PP1055E2 Polypropylene Homopolymer Product Description: A nucleated homopolymer resin with good flowability and antistatic properties. It is designed for molding of media packaging, containers and other articles requiring fast moldi.. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D-638 |
Axiall Suprel® 9422 Rigid PVC, Molding Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with.. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Westlake Plastics Halar® 901 ECTFE Made from HALAR® ethylene-chlorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impa.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ISO 527 |
Polyram RamLloy A001 Nylon 66/Polyethylene Alloy for Injection Molding, Impact Modified Nylon 66/PE Alloy, reduction of water absorption, impact modified, for injection molding applications.Information provided by Polyram. |