Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.65 GPa @Temperature 23.9 °C |
240 ksi @Temperature 75.0 °F |
0° Direction, Dry; 325°F Autoclave; ASTM D638 |
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Commercial Silica Fabric Reinforced Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle.. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Quadrant EPP Symalit® ECTFE Ethylene-Chlorotrifluoroethylene (ASTM Product Data Sheet) |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | |
Saint-Gobain Rulon® E Grade Bearing/Seal PTFE
(discontinued **) Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and .. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 1.66 GPa @Thickness 3.20 mm |
240 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical AP163 ABS, Permanent Anti-Static Feature: Injection Molding, Permanent Anti-StaticApplication: E & E Products (IC tray etc)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Modulus | 1.66 GPa @Thickness 3.20 mm |
240 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Fiberfil® J-68/10/E Polypropylene Copolymer, 10% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Spartech Litho SP-2090 Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
ScanTube ECTFE Tubing Information provided by ScanTube, Inc. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Westlake Plastics Propylux® Polypropylene Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance it abrasion. These properties makes it suitable f.. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
American Polymers API 505 Polystyrene API 505 is an intermediate grade of impact modified polystyrene. This material has exceptional moldability and colorability.Applications: API 505 is widely used in housewares, toys, containers, dis.. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | Tested using a 50 mil. Sheet; ASTM D638 |
Chevron Phillips EB6755 Rubber Modified Polystyrene DescriptionChevron EB6755 is an extrusion grade, high impact polystyrene developed for use in packaging applications. It is designed for exceptional environmental stress-crack resistance and practi.. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Ensinger Hydex™ 202 Rigid Polyurethane (PU) Hydex™ 202 is a totally rigid polyurethane resin that exhibits a broad range of chemical resistance, as well as superior impact and excellent mechanical properties. It can be used for any mechanic.. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Ensinger Tecatron® XP-79 Compression Molded PPS Compound, 70% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D-638 |
Axiall Suprel® 9422 Rigid PVC, Molding Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with.. |
|||
Tensile Modulus | 1.65 - 2.28 GPa | 240 - 330 ksi | ASTM D638 |
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |
|||
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D638 |
Westlake Plastics Halar® 901 ECTFE Made from HALAR® ethylene-chlorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impa.. |