Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.20 GPa | 1190 ksi | |
Plastcom SLOVAMID 6 GF 15 T 25 LTS PA6, 15% glass fibre, 25% mineral filling FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooli.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | |
Plastcom SLOVAMID 6 GF 15 T 25 TS PA6, 15% glass fibre, 25% mineral filling FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooli.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | ISO 527-1/2 |
Radici Radilon® SRCP3010LK (dry) Nylon 6 Heat stabilized glass-fiber reinforced and mineral reinforcedInformation provided by Radici group. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | ISO 527-2 |
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin Features: Ultra high modulus, High heat resistance, excellent adhesion to urethaneApplications: Instrument panel substrates, Brackets, Structural components |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | |
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | |
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | |
LATI Laticonther 52/11 GR/70 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical .. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | ASTM D638 |
Plenco 2308 Phenolic, Granular, Transfer Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | ASTM D638 |
Plenco 2311 Phenolic, Granular, Injection Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | ASTM D638 |
Plenco 4548 Phenolic, Granular, Injection Molded PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP H 0580 GFC Polypropylene, 40% Glass Filled PP homopolymer 40% chemically coupled glass fiberExcellent stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q-X07209 PA410-I-GF40 % Glass Reinforced, Impact Modified |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-2 FWA nat PA*-GF20 Product description: Grivory GV-2 FWA natural is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyami.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-2H black PA*-GF20 Product description: Grivory GV-2H is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide. Grivory.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-2H PA*-GF20 Product description: Grivory GV-2H natural is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide... |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GV 25 HWCP 25% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-2 FWA black 9225 PA*-GF20 Product description: Grivory GV-2 FWA black 9225 is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copoly.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF40 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 40% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Tensile Modulus | 8.20 GPa | 1190 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Conditioned, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 8.20 GPa @Treatment Temp. 70.0 °C, Time 90000 sec |
1190 ksi @Treatment Temp. 158 °F, Time 25.0 hour |
62% rel. humidity |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 8.20 GPa @Temperature 120 °C |
1190 ksi @Temperature 248 °F |
ISO 527-1/-2 |
DSM Stanyl® TS200F10 PA46-GF50 50% Glass Reinforced |