Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | >= 100 g | >= 0.221 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4117N (18401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Chevron Phillips mPact™ D353 m-MDPE Linear Low Density Polyethylene
(discontinued **) Low Density PolyethyleneCustomer Benefits: This metallocene medium density PE for cast film applications offers greater tensile modulus than LLDPE while retaining excellent optical properties.Data p.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D-1709 |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength, 0.7 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D 1709/A |
NOVA Chemicals Novapol® PF-0118-DP Butene Copolymer LLDPE Film Resin PF-0118-DP complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatu.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D 1709/A |
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin PF-0218-B complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D 1709/A |
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin PF-0218-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Dart Drop Test | 100 g | 0.221 lb | |
DuPont™ Sclairfilm® LWS-1 LMDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |
|||
Dart Drop Test | 100 g | 0.221 lb | |
DuPont™ Sclairfilm® LWS-2 LMDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
LyondellBasell Montell 12C01G3 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: .. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene 09X02 is a high performance LLDPE (HP-LLDPE) cast film grade combines ease of processing with low gels and good film strength. Its excellent stretchability makes this grade particularly suited for s.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Iran Petrochemical (PCC) LF0200 Low Density Polyethylene LF0200 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. LF0200 contains antioxidant.Applications: genera.. |
|||
Dart Drop Test | 100 g @Thickness 0.0400 mm |
0.221 lb @Thickness 0.00157 in |
ISO 7765-1 |
Borealis FA6220 Low Density Polyethylene FA6220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for the production of thin blown films. Applications: shrink film, pouches, general packagin.. |
|||
Dart Drop Test | >= 100 g | >= 0.221 lb | 40µm; ASTM D 1709 |
Total Lumicene® M 3410 EP HDPE Film, sheet FINACENE® M 3410 EP is a medium density metallocene based polyethylene resin. FINACENE® M 3410 EP is especially dedicated to film applications where a higher rigidity, good transparency and shrink.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Formosa Plastics Formolene® L62608 Film (Hexene Grade) LLDPE Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil Exact™ 3040 Cast Ethylene-based Plastomer Resin Product Description: Exact 3040 is an ethylene-based hexane copolymer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monolayer and coextrusion cast fi.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B |
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Slot Cast Extrusion Outstanding Drawdown Capability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7046 NT 7 is an ethylene-hexene copolymer, designed f.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM-D1709 |
Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer FL31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for cast film extrusion. Films obtained with this product show a good processing .. |
|||
Dart Drop Test | 100 g | 0.221 lb | gF/50%f; ASTM D1709 |
Braskem LHB118/21AF Blown Film Extrusion Linear Low Density Polyethylene Frozen chicken packages; Meat-based frozen packages.Additives: Antiblock, D, PPA, PEBDInformation provided by Braskem. |
|||
Dart Drop Test | 100 g | 0.221 lb | gF/50%f; ASTM D1709 |
Braskem LL118 Blown Film Extrusion Linear Low Density Polyethylene Description: LL218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and .. |
|||
Dart Drop Test | 100 g | 0.221 lb | g/F50; ASTM D1709 |
Braskem LL218/21 Cast Film Extrusion Linear Low Density Polyethylene Liners, LDPE and HDPE blends; General use packages; Technical films for automatic packaging.Additives: Antiblock, DInformation provided by Braskem. |
|||
Dart Drop Test | 100 g | 0.221 lb | gF/50%f; ASTM D1709 |
Braskem BF0323/12HC Blown Film Extrusion Low Density Polyethylene Shrink films; Automatic packaging of liquid products (FFS).Additives: Antiblock, DInformation provided by Braskem. |
|||
Dart Drop Test | 100 g | 0.221 lb | gF/50%f; ASTM D1709 |
Braskem BF0323HC Blown Film Extrusion Low Density Polyethylene Heavy-duty bags; Agriculture, Coextruded and shrink films for pallets.Information provided by Braskem. |