Chevron Phillips mPact™ D353 m-MDPE Linear Low Density Polyethylene  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips mPact™ D353 m-MDPE Linear Low Density Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Density PolyethyleneCustomer Benefits: This metallocene medium density PE for cast film applications offers greater tensile modulus than LLDPE while retaining excellent optical properties.Data provided by Chevron Phillips Chemical Company, LP.
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
ASTM D1505
Melt Flow 2.5 g/10 min
2.5 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
2 in per min; ASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
2 in per min; ASTM D882
Film Elongation at Break, MD 500 %
500 %
2 in per min; ASTM D882
Film Elongation at Break, TD 500 %
500 %
2 in per min; ASTM D882
Elmendorf Tear Strength MD 100 g
100 g
ASTM D1922
Elmendorf Tear Strength TD 300 g
300 g
ASTM D1922
Dart Drop Test 100 g
0.221 lb
ASTM D1709
Film Tensile Strength at Break, MD 27.0 MPa
3920 psi
2 in per min; ASTM D882
Film Tensile Strength at Break, TD 22.0 MPa
3190 psi
2 in per min; ASTM D882
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM D1003
Gloss 91 %
91 %
45°; ASTM D2457