Polymer Property : Flexural Yield Strength = 179 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 13.0 - 179 MPa
1890 - 26000 psi
Average value: 78.4 MPa Grade Count:230
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Flexural Yield Strength 68.9 - 179 MPa
10000 - 26000 psi
Average value: 91.2 MPa Grade Count:63
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Flexural Yield Strength 84.1 - 179 MPa
12200 - 26000 psi
Average value: 120 MPa Grade Count:21
Overview of materials for Polycarbonate, Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr..
Flexural Yield Strength 124 - 179 MPa
18000 - 26000 psi
Average value: 145 MPa Grade Count:3
Overview of materials for Nylon 11 with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ..
Flexural Yield Strength 72.4 - 179 MPa
10500 - 26000 psi
Average value: 120 MPa Grade Count:20
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
Flexural Yield Strength 55.0 - 179 MPa
7980 - 26000 psi
Average value: 128 MPa Grade Count:37
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..
Flexural Yield Strength 110 - 179 MPa
16000 - 26000 psi
Average value: 143 MPa Grade Count:4
Overview of materials for Acrylic, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o..
Flexural Yield Strength 138 - 179 MPa
20000 - 26000 psi
ASTM D790
Premix Premi-Glas® 1200-28 Polyester SMC  (discontinued **)
Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and..