Mechanical Properties Metric English Comments
Flexural Yield Strength 110 - 193 MPa
16000 - 28000 psi
Average value: 142 MPa Grade Count:27
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Flexural Yield Strength 97.9 - 193 MPa
14200 - 28000 psi
Average value: 139 MPa Grade Count:24
Overview of materials for ABS/Polyester Alloy + GF
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro..
Flexural Yield Strength 82.7 - 193 MPa
12000 - 28000 psi
Average value: 151 MPa Grade Count:6
Overview of materials for Nylon 6, Stainless Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o..
Flexural Yield Strength 13.8 - 193 MPa
2000 - 28000 psi
Average value: 130 MPa Grade Count:68
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Flexural Yield Strength 138 - 193 MPa
20000 - 28000 psi
Average value: 175 MPa Grade Count:3
Overview of materials for PEKK, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate..
Flexural Yield Strength 39.3 - 193 MPa
5700 - 28000 psi
Average value: 132 MPa Grade Count:100
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..
Flexural Yield Strength 138 - 193 MPa
20000 - 28000 psi
Average value: 175 MPa Grade Count:22
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Flexural Yield Strength 55.2 - 193 MPa
8000 - 28000 psi
Average value: 110 MPa Grade Count:28
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max..