Polymer Property : Tensile Strength, Ultimate = 35.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 35.0 - 35.0 MPa

@Temperature 60.0 - 60.0 °C
5080 - 5080 psi

@Temperature 140 - 140 °F
Average value: 35.0 MPa Grade Count:1
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Tensile Strength, Ultimate 35.0 - 35.0 MPa

@Temperature 32.0 - 32.0 °C
5080 - 5080 psi

@Temperature 89.6 - 89.6 °F
Average value: 35.0 MPa Grade Count:1
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Tensile Strength, Ultimate 13.0 - 35.0 MPa
1890 - 5080 psi
Average value: 24.5 MPa Grade Count:32
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..
Tensile Strength, Ultimate 25.0 - 35.0 MPa
3630 - 5080 psi
ASTM D638
Zeus PFA Tubing
PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar..
Tensile Strength, Ultimate 20.0 - 35.0 MPa
2900 - 5080 psi
ASTM D638
Zeus PTFE Tubing
Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,..
Tensile Strength, Ultimate 4.00 - 35.0 MPa
580 - 5080 psi
ASTM D638
Dow Engage® Polyolefin Elastomer
Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. ..
Tensile Strength, Ultimate 15.0 - 35.0 MPa
2180 - 5080 psi
ATG s.r.l. AU-EU Polyurethane Rubber
Tensile Strength, Ultimate 27.0 - 35.0 MPa
3920 - 5080 psi
ISO 527
BASF Ecovio® C2224 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..
Tensile Strength, Ultimate 13.0 - 35.0 MPa
1890 - 5080 psi
Average value: 23.9 MPa Grade Count:12
Overview of materials for Polypropylene with 10% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are ..