Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 35.2 MPa @Temperature 23.9 °C |
5100 psi @Temperature 75.0 °F |
Short Beam; Dry; 8HS form; ASTM D5379 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® 301-2 Optically Transparent Epoxy Product Description: EPO-TEK® 301-2 is a two component optical, medical, and semiconductor grade epoxy resin, with low viscosity, long pot-life, and good handling characteristics.Advantages & Appli.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® 320 Optical, Opaque Epoxy Product Description: EPO-TEK® 320 is a two component, black-colored and optically opaque epoxy designed for optical, medical, and optoelectronic packaging of semiconductor devices and components. .. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® 353ND Black High Temperature Epoxy Product Description: EPO TEK® 353ND Black is a a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applicationsAdvantages & Application Notes: EPO T.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy Product Description: EPO-TEK® 353ND is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. It is one of the most popular EPO-TEK® bra.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® 353ND-T Black High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T Black is a two component, high temperature, thixotropic epoxy for fiber optic, PCB and various medical applications. Advantages & Application Notes: This produ.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® 353ND-T High Temperature Thixotropic Epoxy Product Description: EPO TEK® 353ND-T is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. Advantages & Application Notes: Suitable for fiber op.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® 353ND-T1 High Temperature Thixotropic Epoxy Material Description: A two component, thixotropic and high temperature epoxy designed for fiber optic, electronics and medical applications. It is a more viscous alternative to EPO-TEK® 353ND-T.I.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® 353ND-T4 Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T4 is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. This is a higher viscosity version of EPO-TEK® 353.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® 353ND-T5 High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T5 is an intermediate viscosity version of EPO-TEK® 353ND and EPO-TEK® 353ND-T. It was designed for high temperature applications in fiber optics, electronics .. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® CF6-2 High Temperature Epoxy Product Description: EPO-TEK® CF6-2 is a two component, high temperature and high Tg epoxy designed for fiber optic packaging. Advantages & Application Notes: The low viscosity nature allows for wi.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® EE149-6 Epoxy Material Description: A single component, silver-filled, B-stageable epoxy designed for semiconductor flip chip packaging or hybrid micro-electronic substrate attach or lid-sealing.Information Provi.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® H27D Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H27D is a two component, silver-filled epoxy adhesive designed for semiconductor and hybrid-microelectronic packaging applications.Advantages & Application Notes: Rheo.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® H54 High Temperature Epoxy Product Description: EPO-TEK® H54 is a two component, high Tg, electrically and thermally insulating epoxy adhesive for general bonding and high temperature packaging in medical, hybrid, and optica.. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® OE101 Two Component Epoxy Material Description: A two component epoxy designed for low stress applications in fiber optic packaging, opto-electronics and semiconductors. It is a lower modulus version of EPO-TEK® 353ND.Inf.. |
|||
Shear Strength | 35.2 MPa | 5100 psi | Die |
Epoxy Technology EPO-TEK® OE121 Black Epoxy Adhesive Material Description: A two component, low temperature curing epoxy adhesive designed for semiconductor flip chip underfill. It is color coded black for visual ID during the underfilling process. .. |
|||
Shear Strength | >= 35.2 MPa | >= 5100 psi | Die |
Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy Product Description: EPO-TEK® OE188 is a low CTE, designed for semiconductor and fiber optic applications. Advantages & Application Notes: Paste-like viscosity allows for application by dispensing.. |
|||
Shear Strength | 35.2 MPa | 5100 psi | Overlap, RT at 50% RH for 30 days |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |