Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis HE125MO Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis HE125MO Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HE125MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by good flow properties and high stiffness in and is specially suitable for high-speed injection molding of articles demanding easy flow. Its very good organoleptic properties allows this grade to be used with any master batch without discoloring problems. Applications: house ware and thin wall packaging, articles with rather long and narrow flow lengths.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.908 g/cc
0.0328 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ISO 2039-2
Tensile Strength, Yield 34.5 MPa
5000 psi
50mm/min; ISO 527-2
Elongation at Yield 9.0 %
9.0 %
50mm/min; ISO 527-2
Flexural Modulus 1.55 GPa
225 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 220 - 260 °C
428 - 500 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity high
Users viewing this material also viewed the following: