Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.7 GPa | 1550 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Flexural Modulus | 10.69 GPa | 1550 ksi | ASTM D790 |
Covestro Petlon® 4630 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Electrical Properties, High Heat and Chemical ResistanceApplications: Connectors, Relays, Switches, Automotive (Under Hood), AppliancesProcessing: Injection Molding.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
PolyOne LubriOne™ NJ-30CF/15T-2S Nylon 12
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 C14 BK 14% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF30 FR BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 HS L 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizerInformati.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 L 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PPS/F GF/M35 X 35% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC LNP* Thermocomp* Lexan_LGN5030 compound is a glass reinforced. Flame retardant. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGK5020 compound is a glass reinforced, flame retardant material. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 15% Filler by WeightAdditive: LubricantFeatures: Flame Retardant and LubricatedAppearance: BlackInformation.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES Luriblend® PPA GF30 SL2 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided b.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Plenco 1581 Polyester, Pellet, Injection Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM-D790 |
Polyram Polytron A30N02 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam RF0023K PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0023K is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding, Crosslinkable under Beta or Gamma RadiationInformation provided by Euros.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ISO 178 |
BASF Ultramid® 66 H2 G/35-V0KB NAT 0046 35% Glass Filled PA66 (Dry) Description: Ultramid 66 H2 G/35-V0KB NAT0046 is a 35% glass reinforced, heat stabilized injection molding grade. It is a V-0 self-extinguishing grade, with phosphorous. It offers good flowability a.. |