Mechanical Properties Metric English Comments
Flexural Modulus 6.89 - 17.2 GPa
1000 - 2500 ksi
Average value: 9.08 GPa Grade Count:6
Overview of materials for PPE/PPO + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr..
Flexural Modulus 12.4 - 17.2 GPa
1800 - 2500 ksi
Average value: 14.6 GPa Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Flexural Modulus 4.48 - 17.2 GPa
650 - 2500 ksi
Average value: 7.75 GPa Grade Count:18
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
Flexural Modulus 1.21 - 17.2 GPa
175 - 2500 ksi
Average value: 7.83 GPa Grade Count:15
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
Flexural Modulus 7.90 - 17.2 GPa
1150 - 2500 ksi
Average value: 13.9 GPa Grade Count:111
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Flexural Modulus 6.55 - 17.2 GPa
950 - 2500 ksi
Average value: 11.1 GPa Grade Count:7
Overview of materials for Nylon 11 + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp..
Flexural Modulus 4.83 - 17.2 GPa
700 - 2500 ksi
Average value: 10.4 GPa Grade Count:24
Overview of materials for Polyphthalamide (PPA), Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a..