Flexural Modulus 13.4 GPa
1940 ksi
Plastcom SLOVASTER® B1 GF 45 PBT, 45% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 45% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Flexural Modulus 13.4 GPa
1940 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP LCL33EXQ PEEK
LNP* LUBRICOMP* LCL33EXQ is a compound based on Polyetheretherketone containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Easy Molding.
Flexural Modulus 13.4 GPa
1940 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Lubricomp OFG26XXP PPS - Linear
LNP* Lubricomp* OFG26XXP is a compound based on Linear PPS containing Glass Fiber and Graphite Powder. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for..
Flexural Modulus 13.4 GPa
1940 ksi
ISO 178
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
Flexural Modulus 13.4 GPa
1940 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DEL36 PC (Europe-Africa-Middle East)
LNP* STATKON* DEL36 is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated.
Flexural Modulus 13.4 GPa
1940 ksi
ASTM D790
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP), 30% Glass Fiber
Xydar® G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology.The moldab..
Flexural Modulus 13.4 GPa
1940 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS (Asia Pacific)
LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber.This product is also known as Thermocomp* OF-1008.
Flexural Modulus 13.4 GPa
1940 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP OF008AH PPS - Branched
LNP* THERMOCOMP* OF008AH is a compound based on PPS - Branched resin containing 40% Glass Fiber. Added features of this grade are: Healthcare.
Flexural Modulus 13.4 GPa
1940 ksi
ISO 178
SABIC Innovative Plastics LNP Thermocomp OF008E PPS
LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the A..
Flexural Modulus 13.4 GPa
1940 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - LINEAR
LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing 40% Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 13.4 GPa
1940 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS (Asia Pacific)
LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 13.4 GPa
1940 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI
LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced.
Flexural Modulus 13.4 GPa
1940 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched
LNP* THERMOCOMP* OF008A is a compound based on PPS - Branched resin containing 40% Glass Fiber.
Flexural Modulus 13.4 GPa
1940 ksi
ASTM D790
A. Schulman ComAlloy Voloy® 682 Nylon 6/6, Glass Fiber, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 13.4 GPa
1940 ksi
ASTM D790
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)  (Unverified Data**)
Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili..
Flexural Modulus 13.4 GPa
1940 ksi
ISO 178
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature..
Flexural Modulus 13.4 GPa
1940 ksi
ASTM D790
LNP Thermocomp® UF-1008 Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..