Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.02 - 4.10 GPa | 148 - 595 ksi | Average value: 2.08 GPa Grade Count:301 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Flexural Modulus | 1.40 - 4.10 GPa | 203 - 595 ksi | Average value: 2.51 GPa Grade Count:119 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Flexural Modulus | 1.12 - 4.10 GPa | 163 - 595 ksi | Average value: 2.05 GPa Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Wood Filled". Each property range of values reported is minimum and ma.. |
|||
Flexural Modulus | 3.60 - 4.10 GPa | 522 - 595 ksi | ASTM D790 |
Zeus PEEK Tubing PEEK (polyetheretherketone) is a high-performance engineered polymer with excellent endurance to heat and one of the highest strength-to-weight ratios of any thermoplastic. This material can be used.. |