Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 130 MPa @Temperature 175 °C |
18900 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Flexural Strength | 130 MPa @Strain 3.50 % |
18900 psi @Strain 3.50 % |
ISO 178 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Flexural Strength | 130 MPa @Strain 3.50 % |
18900 psi @Strain 3.50 % |
ISO 178 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Flexural Strength | 130 MPa @Temperature 175 °C |
18900 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Flexural Strength | 130 MPa @Temperature 175 °C |
18900 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
Flexural Strength | 130 MPa @Strain 3.50 %, Temperature 23.0 °C |
18900 psi @Strain 3.50 %, Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Flexural Strength | 130 MPa @Strain 3.50 %, Temperature 23.0 °C |
18900 psi @Strain 3.50 %, Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Flexural Strength | 130 MPa @Strain 3.50 % |
18900 psi @Strain 3.50 % |
ISO 178 |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
Flexural Strength | 130 MPa @Strain 6.50 % |
18900 psi @Strain 6.50 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding PA 66, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Flexural Strength | 130 MPa @Strain 5.00 % |
18900 psi @Strain 5.00 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
Flexural Strength | 130 MPa @Strain 5.50 % |
18900 psi @Strain 5.50 % |
ISO 178 |
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers PA 6-Copolymer, 15% glass fibers, injection molding, impact modified |
|||
Flexural Strength | 130 MPa @Strain 6.00 % |
18900 psi @Strain 6.00 % |
ISO 178 |
Lanxess Durethan® A 30 H3.0 000000 Nylon 66 PA 66, non reinforced, injection molding, heat-ageing stabilized |
|||
Flexural Strength | 130 MPa @Strain 5.50 % |
18900 psi @Strain 5.50 % |
ISO 178 |
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties |
|||
Flexural Strength | 130 MPa @Temperature 23.0 °C |
18900 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.5%); ASTM-D790 |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 130 MPa @Temperature -40.0 °C |
18900 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.5%); ASTM-D790 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 130 MPa @Temperature 80.0 °C |
18900 psi @Temperature 176 °F |
Practical Use (Water Absorption 1.75%); ASTM-D790 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 130 MPa @Temperature 80.0 °C |
18900 psi @Temperature 176 °F |
Practical Use; ASTM-D790 |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 130 MPa @Temperature 80.0 °C |
18900 psi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 130 MPa @Temperature 23.0 °C |
18900 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.9%); ASTM-D790 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 130 MPa @Temperature 23.0 °C |
18900 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 130 MPa @Temperature -40.0 °C |
18900 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 130 MPa @Temperature -40.0 °C |
18900 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 130 MPa @Treatment Temp. 100 °C, Time 3600 sec |
18900 psi @Treatment Temp. 212 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica.. |