Mechanical Properties Metric English Comments
Flexural Strength 130 MPa

@Temperature 175 °C
18900 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c..
Flexural Strength 130 MPa

@Strain 3.50 %
18900 psi

@Strain 3.50 %
ISO 178
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
Flexural Strength 130 MPa

@Strain 3.50 %
18900 psi

@Strain 3.50 %
ISO 178
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou..
Flexural Strength 130 MPa

@Temperature 175 °C
18900 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
Flexural Strength 130 MPa

@Temperature 175 °C
18900 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont..
Flexural Strength 130 MPa

@Strain 3.50 %,
Temperature 23.0 °C
18900 psi

@Strain 3.50 %,
Temperature 73.4 °F
ISO 178
Victrex® PEEK 90G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
Flexural Strength 130 MPa

@Strain 3.50 %,
Temperature 23.0 °C
18900 psi

@Strain 3.50 %,
Temperature 73.4 °F
ISO 178
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
Flexural Strength 130 MPa

@Strain 3.50 %
18900 psi

@Strain 3.50 %
ISO 178
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, ..
Flexural Strength 130 MPa

@Strain 6.50 %
18900 psi

@Strain 6.50 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding
PA 66, non-reinforced, injection moldingInformation provided by LANXESS.
Flexural Strength 130 MPa

@Strain 5.00 %
18900 psi

@Strain 5.00 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified
PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS.
Flexural Strength 130 MPa

@Strain 5.50 %
18900 psi

@Strain 5.50 %
ISO 178
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers
PA 6-Copolymer, 15% glass fibers, injection molding, impact modified
Flexural Strength 130 MPa

@Strain 6.00 %
18900 psi

@Strain 6.00 %
ISO 178
Lanxess Durethan® A 30 H3.0 000000 Nylon 66
PA 66, non reinforced, injection molding, heat-ageing stabilized
Flexural Strength 130 MPa

@Strain 5.50 %
18900 psi

@Strain 5.50 %
ISO 178
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral
PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties
Flexural Strength 130 MPa

@Temperature 23.0 °C
18900 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.5%); ASTM-D790
Toyobo GLAMIDE® T-402 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 130 MPa

@Temperature -40.0 °C
18900 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.5%); ASTM-D790
Toyobo GLAMIDE® T-521 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 130 MPa

@Temperature 80.0 °C
18900 psi

@Temperature 176 °F
Practical Use (Water Absorption 1.75%); ASTM-D790
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 130 MPa

@Temperature 80.0 °C
18900 psi

@Temperature 176 °F
Practical Use; ASTM-D790
Toyobo GLAMIDE® T-669VGB Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 130 MPa

@Temperature 80.0 °C
18900 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 130 MPa

@Temperature 23.0 °C
18900 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.9%); ASTM-D790
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 130 MPa

@Temperature 23.0 °C
18900 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-835TC Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 130 MPa

@Temperature -40.0 °C
18900 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 130 MPa

@Temperature -40.0 °C
18900 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 130 MPa

@Treatment Temp. 100 °C,
Time 3600 sec
18900 psi

@Treatment Temp. 212 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica..