Mechanical Properties Metric English Comments
Flexural Strength 260 MPa

@Strain 4.00 %
37700 psi

@Strain 4.00 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 260 MPa

@Temperature 23.0 °C
37700 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-402 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 260 MPa

@Temperature -40.0 °C
37700 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-602G30 MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 260 MPa

@Temperature 23.0 °C
37700 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.25%); ASTM-D790
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 260 MPa

@Temperature 23.0 °C
37700 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
Toyobo GLAMIDE® T-663G50A MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 260 MPa

@Temperature 23.0 °C
37700 psi

@Temperature 73.4 °F
50%RH; ISO 178
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont ..
Flexural Strength 260 MPa

@Temperature 23.0 °C
37700 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..