Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 70.0 °C @Load 1.00 kg |
158 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® MP 34 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding Greenflex MP 34 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MP 34 combines high fluidity with high elasticity.Main Applications: Gree.. |
|||
Vicat Softening Point | 70.0 °C @Load 5.10 kg |
158 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® CS 35FL (dry) Nylon 6/66 Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® TPU-7682 Thermoplastic polyurethane, with carbon fiber Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® TPE-7829 Thermoplastic elastomer, with PTFE Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K.. |
|||
Vicat Softening Point | 70.0 °C @Load 5.00 kg |
158 °F @Load 11.0 lb |
|
LATI Latene® EP 7 TES/30 PP Copolymer, 30% Talc filled Polypropylene copolymer (PPc) based compound. Aesthetic talc. Very good surface appearance. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ISO 306 |
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Lushan M-2 Adhesive Resin for Barrier Container and Tube Adhesive resin Lushan series for barrier container and tube is used for bonding a wide variety of materials, It’s most often used to adhering PE and EVOH, PP and EVOH, etc. Adhesive resins Lush.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
SK Chemicals SKYTHANE® CR180A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
SK Chemicals SKYTHANE® R180A C series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Teknor Apex Laripur® LPR 7560EG Thermoplastic Polyurethane Features: - Excellent performance under extreme and aggressive environments
- Superior abrasion and cut resistance
- Resistance to chemical, microbial attack and hydrolysis
- Excellent flexibility a.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
UBE V115 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | D1525 |
Westlake EF522 12% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF522 is an ethylene vinyl acetate copolymer with 12% VA. EF522 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength m.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 7612 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7612 is a nucleated and controlled-rheology heterophasic copolymer. PPC 7612 is characterized by a good balance between rigidity and impact resistance and has excellent antistatic.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 7760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7760 is a heterophasic copolymer. PPC 7760 is characterized by medium fluidity offering a combination of ease of processing and excellent impact properties in applications ranging.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 9760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9760 is heterophasic copolymer. PPC 9760 is characterized by improved stiffness, creep resistance and high impact resistance. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 12712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane Features: Displays Low Temperature Flexibility and Abrasion Resistance.Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for LaminationAvailable in Americas and AsiaInfo.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50°C/hr; 50N |
Arkema Group Nakan® RMA 705 N PVC, Rigid Injection Molding Grade NAKAN RMA 705 N L is a rigid polyvinyl chloride compound developed for injection molding of various medium impact resistance applications.ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR7560 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | |
BASF Novolen® 2348 TC Polypropylene Grade with nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 70.0 °C @Load 0.999 kg |
158 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 6200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 6200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties (reactivity, fluidity), LOTADER 62.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 49 N; ISO 306 |
A.D. Compound Adene NCFAG Copolymer 20% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Arkema Group Orevac® 9314 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Blown film coextrusionInformation provided by Arkema Group |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 10712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 10712 is a nucleated and controlled-rheology heterophasic copolymer. PPC 10712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. |
|||
Vicat Softening Point | 70.0 - 80.0 °C | 158 - 176 °F | Average value: 76.7 °C Grade Count:3 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |