Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 757 G Q43 White 36609 ASA
Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between..
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 757 G UV White 37019 ASA
Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between..
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 757 R Colored ASA
Description: General-purpose grade for injection molding with high stiffness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 776 S Colored ASA
Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j..
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 776 S UV ASA
Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j..
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 777 K UV Black 56625 ASA
Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 778 Q42 Colored ASA
Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan..
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 778 TE Black 25991 ASA
Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 778 TE UV Colored ASA
Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 778 UV Colored ASA
Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan..
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 796 M Colored ASA
Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 797 S UV White 33999 Q455 ASA
Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S 797 S White 35962 ASA
Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S KR 2859 ASA
Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S KR 2859 UV ASA
Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Terluran® HH-106 Q109 Colored ABS
Description: Injection-molding grade with high resistance to heat deformation and impact, with improved surface quality suitable for automotive applications.Information provided by STYROLUTION, whic..
CTE, linear, Parallel to Flow 70.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Terluran® HH-112 Q109 ABS
Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
CTE, linear, Parallel to Flow 70.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS
Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Terluran® SP-6 ABS
Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Terlux® 2802 TR Q434 Transparent MABS
Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
CTE, linear, Parallel to Flow 60.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
33.3 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Dry)
Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for..
CTE, linear, Parallel to Flow 20.0 - 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
11.1 - 61.1 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT
Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so..