Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 102 °C | 216 °F | Internal Method |
Polimeri Europa Greenflex® FF 35 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 35 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. The resin shows good strechability and sealability.Main Applications: Greenflex FF 35 is suitable for flexibl.. |
|||
Melting Point | 102 °C | 216 °F | Internal method |
Polimeri Europa Riblene® MY 00 Low Density Polyethylene - Injection Molding Riblene MY 00 is a very high flowability low density polyethylene resin (LDPE).Main Applications: Riblene MY 00 is suitable for hot melts.Information provided by Polimeri Europa. |
|||
Melting Point | 102 - 110 °C | 216 - 230 °F | |
Pau Tai Lead stearate, Monomer Stabilizer Stabilizer with low price, excellent lubricity with cadmium, barium.Applications: Rigid plate, injection soft products. |
|||
Melting Point | 102 °C | 216 °F | Exxon Method |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process.. |
|||
Melting Point | 102 °C | 216 °F | Exxon Method |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Injection Molding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be injection molded to produce pliable parts. It can also be used for making.. |
|||
Melting Point | 102 °C | 216 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
(discontinued **) 7 wt% Acrylic Acid.Nucrel® 30707SR is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio.. |
|||
Melting Point | 102 °C | 216 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 3095 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 102 °C | 216 °F | Exxon Method |
ExxonMobil Escorene® CR-5810 EVA Resin, for High Cling Stretch Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A tackified Ethylene Vinyl Acetate resin for blown or cast stretch film.Applications: Packing films (cling). Data for film properties below based o.. |
|||
Melting Point | 102 °C | 216 °F | ASTM D3418 |
LyondellBasell Microthene® G MN70100 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melting Point | 102 °C | 216 °F | ASTM D3418 |
LyondellBasell Microthene® G MN71400 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melting Point | 102 - 108 °C | 216 - 226 °F | |
Indium Corp. Indalloy 52 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 102 °C | 216 °F | ISO 3146 |
Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate Lucofin 1400HN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN Powder is softer and more flexible than ethy.. |
|||
Melting Point | 102 °C | 216 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Melting Point | 102 °C | 216 °F | by DSC; ASTM D3418 |
Westlake EBAC® Plus SP1903 18% Ethylene Butyl Acrylate Copolymer Westlake EBAC® SP1903 is an 18% EBA copolymer designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1903 provides excel.. |
|||
Melting Point | 102 °C | 216 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating 7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion .. |
|||
Melting Point | 102 °C | 216 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 306.38 High Clarity, High Impact Film Resin LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical |
|||
Melting Point | 102 °C | 216 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 306.57 High Clarity, High Impact Film Resin LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical |
|||
Melting Point | 102 °C | 216 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 306.75 High Clarity, High Impact Film Resin LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical |
|||
Melting Point | 102 °C | 216 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 317.09 Film Resin LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon.. |
|||
Melting Point | 102 °C | 216 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 317.87 Film Resin LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon.. |
|||
Melting Point | 102 °C | 216 °F | 10°C/min |
Arkema Group Evatane® 1005 VN 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible, very transparent film with high strength, shrinking at low temperature. Examples: curtain stretch, coextrusion, .. |
|||
Melting Point | 102 °C | 216 °F | DSC |
Arkema Group LOTADER® 6200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 6200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties (reactivity, fluidity), LOTADER 62.. |
|||
Melting Point | 102 °C | 216 °F | Freezing Point; ASTM D3418 |
DuPont™ Fusabond® E226 Polymer Modifier DuPont™ Fusabond® E226 is a anhydride modified polyethylene. Uses: Wire & Cable Applications Polymer Modifier Fusabond E226 resin conforms with the Code of Federal Regulations, Title 21, Paragra.. |
|||
Melting Point | 102 - 103 °C | 216 - 217 °F | |
Indium Corp. Indalloy 45 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 102 °C | 216 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 3933 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 102 °C | 216 °F | |
Mitsui EXCEREX™ 30200B(T) Polymer Processing Aid EXCEREX™ is an innovative processing improvement agent created with metallocene catalysis technology. EXCEREX™ gains in a number of ares simultaneously, including faster processing speeds, lower .. |