Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 86.0 °C | 187 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 2014 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 86.1 °C | 187 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil ESCOR™ AT 310 Extrusion Coating Resin
(discontinued **) ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo.. |
|||
Melting Point | 86.0 °C | 187 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3174 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Cast Film
(discontinued **) 18 wt% Vinyl Acetate.Elvax® 3174 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 86.0 °C | 187 °F | Exxon Method |
ExxonMobil Escorene® LD-725 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 18% vinyl acetate copolymer designed for specialty film and compounding applications. Outstanding sealability and low modulus are key attributes.. |
|||
Melting Point | 86.0 °C | 187 °F | ASTM D3418 |
Petroquimica Triunfo Tritheva® PN 2021 EVA Copolymer The Tritheva® PN 2021 resin is an Ethylene-Vinyl Acetate copolymer (EVA) mainly used for the production of crosslinked/expanded plates and other parts. This is an easy processing product with high .. |
|||
Melting Point | 86.0 °C | 187 °F | Exxon Method |
ExxonMobil Iotek® 7610 Zinc Ionomer
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low melt index zinc ionomer made from an ethylene acrylic acid base polymer. It is designed to have high durability, resilience and impact streng.. |
|||
Melting Point | 86.0 °C | 187 °F | Exxon Method |
ExxonMobil Iotek® 8610 Sodium Ionomer
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low melt index sodium ionomer made from an ethylene acrylic acid base polymer. It is designed to have high durability, resilience and impact stre.. |
|||
Melting Point | 86.0 °C | 187 °F | ASTM D3418 |
LyondellBasell Microthene® G MU76000 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melting Point | 86.0 °C | 187 °F | DSC |
Silon Tabond 2001 Adhesive Resin TABOND 2001 is EVA modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.Characteristics: • Stron.. |
|||
Melting Point | 86.0 °C | 187 °F | Kofler; SRTM 3022-9 |
Lubrizol Estane® UB410A Thermoplastic Polyurethane Type: Estane® UB410 is a Shore 70A, polyester based, hot melt adhesive with excellent low temperature flexibility thermoplastic polyurethane (TPU).Uses: Extrusion, Powder Coating.Available in Europ.. |
|||
Melting Point | 86.0 °C | 187 °F | TRN-14 |
Tipco Tipcolite® TPF 1119 - Latex Modified Phenolic Resin having 26 mm Norton Flow with 9% Hexamine Latex Modified Phenolic Resin having 26mm Norton Flow, in Powder FormApplications: Automotive & IndustrialProcessing: BrakeliningInformation provided by the Manufacturer, Tipco Industries Ltd.,
Indi.. |
|||
Melting Point | 86.0 °C | 187 °F | by DSC; ASTM D3418 |
Westlake EBAC® SP1802 22.5% Ethylene Butyl Acrylate Copolymer Westlake EBAC® SP1802 is a 22.5% EBA copolymer designed for blown film, tie-layer, coextrusions and blending where flexibility and strength are important. SP1802 provides excellent elasticity and l.. |
|||
Melting Point | 86.0 °C | 187 °F | Peak; Westlake Method |
Westlake Elevate™ EM518 18.5% Ethylene Vinyl Acetate Copolymer Westlake Elevate™ EM518 resin is an 18.5% EVA copolymer designed for injection molding, compounding, and foam. It has excellent low temperature brittleness properties, melt strength, and flexibilit.. |
|||
Melting Point | 86.0 °C | 187 °F | DSC; ASTM-D3418 |
Westlake EMAC® SP2404 18.5% EMA Copolymer Westlake EMAC� SP2404 is a 18.5% EMA copolymer designed for blown film, tie-layer, coextrusions, and blending where flexibility and strength are important. SP2404 provides excellent elasticity .. |
|||
Melting Point | 86.0 °C | 187 °F | DSC |
DuPont™ Surlyn® 9120 Ionomer Resin, Zinc Surlyn® 9120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melting Point | 86.0 °C | 187 °F | DSC |
DuPont™ Surlyn® 9910 Ionomer Resin, Zinc Surlyn® 9910 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melting Point | 86.1 °C | 187 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® LD 720.01 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Melting Point | 86.1 °C | 187 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® LD 720.62 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Melting Point | 86.0 °C | 187 °F | DSC |
Arkema Group OREVAC® 9318 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Melting Point | 86.0 °C | 187 °F | ASTM-D3418 |
Braskem Evateno® 3019 PE EVA Foam Copolymer Evateno® 3019 PE is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content. Evateno® 3019 PE is an easy processing and crosslinkable product with high compatibility with oth.. |
|||
Melting Point | 86.0 °C | 187 °F | ASTM-D3418 |
Braskem Evateno® 8019 PE EVA Foam Copolymer The Evateno® 8019 PE is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium Vinyl-Acetate content. Evateno® 8019 PE is an easy processing and crosslinkable product with high compatibility with.. |
|||
Melting Point | 86.0 °C | 187 °F | ASTM-D3418 |
Braskem PN2021 EVA Foam Copolymer PN2021 is an Ethylene-Vinyl Acetate (EVA) copolymer mainly used for the production of crosslinked/expanded plates and other parts. It is a product with easy processability and high compatibility wit.. |
|||
Melting Point | 86.0 °C | 187 °F | 10°C/min |
Arkema Group Evatane® 1080 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets, medical.ISO data provided by the manufacturer, Arkema. |
|||
Melting Point | 86.0 °C | 187 °F | Exxon Method |
ExxonMobil Escorene® LD-730 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |
|||
Melting Point | 86.0 °C | 187 °F | Exxon Method |
ExxonMobil Escorene® UL-7560 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 18% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melting Point | 86.1 °C | 187 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil ESCOR™ AT 310 Molding, extrusion and compounding resin