Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 112 °C | 234 °F | Internal method |
Polimeri Europa Riblene® FF 20 Low Density Polyethylene - Blown Film Extrusion Riblene FF 20 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FF 20 is characterized by a good melt strength leading to a good bubble stability.. |
|||
Melting Point | 112 °C | 234 °F | Internal method |
Polimeri Europa Riblene® FF 22 Low Density Polyethylene - Blown Film Extrusion Riblene FF 22 is a high molecular weight low density polyethylene (LDPE), with added slip agent, suitable for blown film extrusion. Riblene FF 22 is characterized by a good melt strength leading to.. |
|||
Melting Point | 112 °C | 234 °F | Internal method |
Polimeri Europa Riblene® MP 30 R Low Density Polyethylene - Injection Molding Riblene MP 30 R is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MP 30 R are characterized by a medium rigidity.Main Applications: Riblene MP 30 R is suitable for in.. |
|||
Melting Point | 112 °C | 234 °F | Internal method |
Polimeri Europa Riblene® MP 31 Low Density Polyethylene - Injection Molding Riblene MP 31 is a medium fluidity low density polyethylene resin (LDPE), with added slip agent.Parts made by Riblene MP 31 are characterized by a medium rigidity.Main Applications: Riblene MP 31 i.. |
|||
Melting Point | 112 °C | 234 °F | Internal method |
Polimeri Europa Riblene® MP 31 R Low Density Polyethylene - Injection Molding Riblene MP 31 R is a medium fluidity low density polyethylene resin (LDPE), with added slip agent.Parts made by Riblene MP 31 R are characterized by a medium rigidity.Main Applications: Riblene MP .. |
|||
Melting Point | 112 °C | 234 °F | Internal method |
Polimeri Europa Riblene® MP 30 Low Density Polyethylene - Injection Molding Riblene MP 30 is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MP 30 are characterized by a medium rigidity.Main Applications: Riblene MP 30 is suitable for injectio.. |
|||
Melting Point | 112 °C | 234 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 071.MU Blown Film Resin
(discontinued **) LD 071 series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, toughness, burn-through re.. |
|||
Melting Point | 112 °C | 234 °F | Exxon Method |
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a.. |
|||
Melting Point | 112 °C | 234 °F | ISO 11357-3 |
Total Lacqtene® FD 0270 LDPE, blown film, compounding, injection molding
(discontinued **) Low density radical polyethylene made by high pressure process. Temperature profile (°C) for injection molding: 200 to 260Information provided provided by Total Petrochemicals.Total Petrochemicals .. |
|||
Melting Point | 112 °C | 234 °F | ISO 11357-3 |
Total Lacqtene® FB 3010 LDPE blown film
(discontinued **) Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 180 to 220°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes form.. |
|||
Melting Point | 112 °C | 234 °F | DSC |
Silon Tabond 2002 Adhesive Resin TABOND 2002 is ethylene-octene Plastomer / LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.. |
|||
Melting Point | 112 °C | 234 °F | ISO 11357-3 |
Borealis FT5230 Low Density Polyethylene FT5230 is a Low Density Polyethylene for Film Extrusion. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications: .. |
|||
Melting Point | 112 °C | 234 °F | ISO 11357-3 |
Borealis FT5231 Low Density Polyethylene FT5231 is a Low Density Polyethylene for blown film. Tubular technology. Contains Antioxidant. This grade is developed for the production of packaging film with good optical properties for medium d.. |
|||
Melting Point | 112 °C | 234 °F | ISO 11357-3 |
Borealis FT5232 Low Density Polyethylene FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op.. |
|||
Melting Point | 112 °C | 234 °F | ISO 11357-3 |
Borealis FT5236 Low Density Polyethylene FT5236 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes anti-block, antioxidant and medium slip additives. Applications FT5236 has been developed especially for applic.. |
|||
Melting Point | 112 °C | 234 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 112 °C | 234 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 4157 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Melting Point | 112 °C | 234 °F | ASTM D3417, ISO 3146 |
DuPont™ Appeel® 45D747 Polyolefin Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion.. |
|||
Melting Point | 112 °C | 234 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 071.LQ Blown Film Resin L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou.. |
|||
Melting Point | 112 °C | 234 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 071.LR Blown Film Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Melting Point | 112 °C | 233 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 123.LN General Purpose Clarity Film Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
Melting Point | 112 °C | 233 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 124.MS General Purpose Clarity Film Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Melting Point | 112 °C | 234 °F | Dow Method (DSC) |
Dow 611A Low Density Polyethylene (LDPE) A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Melting Point | 112 - 124 °C | 234 - 255 °F | Average value: 121 °C Grade Count:16 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m.. |
|||
Melting Point | 112 °C | 234 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 4107 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 112 °C | 234 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 41E557 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |